Superalloy Supplier Certification (EN 10204), applied to Hastelloy X (N06002): verified numbers first, then the reasoning a specifier applies to Hastelloy X. A RAS Thermal reference page on superalloy supplier certification (en 10204).
Hastelloy X is a nickel-chromium-iron-molybdenum alloy designed for high-temperature strength and exceptional oxidation resistance.
As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.
What Superalloy Supplier Certification (EN 10204) means for Hastelloy X
What fixes superalloy supplier certification (en 10204) for Hastelloy X (N06002) is the verified envelope (8.22 g/cm³, 1100 °C) read against gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.
| Property | Hastelloy X |
|---|---|
| Grade | Hastelloy X (N06002) · GB GH3536 |
| Density | 8.22 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | Gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube |
| Standards | AMS 5536, AMS 5754, ASTM B435, ASTM B572 |
Specification signals
Ask for 3.1 and the manufacturer attests the heat chemistry for Hastelloy X, ask for 3.2 and a third party stands beside the release. In practice the applications list confirms the fit: Hastelloy X is specified for gas turbine combustion chambers and afterburner components, not as a universal filler.
- The feature that separates Hastelloy X from its nearest neighbours is specific: Resistant to carburization and nitriding. Hold the Hastelloy X certificate to proving it, not asserting it.
In practice
Against AMS 5536 / AMS 5754 (GB GH3536), the certificate proves the grade by OES chemistry, not a generic datasheet. Which is how gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C stays provable end to end.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy supplier certification (en 10204) resolve for Hastelloy X?
Hastelloy X is proven on paper by EN 10204, with 3.1 carrying the heat’s own chemistry and 3.2 adding an independent witness. Against AMS 5536 / AMS 5754 (GB GH3536), the certificate proves the grade by OES chemistry, not a generic datasheet.
What is Hastelloy X best used for?
Hastelloy X is stocked for gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C; the documented edge is that the combustion-zone standard, oxidation resistant to 1100 °C with good fabricability.
What forms is Hastelloy X available in?
Stocked forms: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube.
What standards does Hastelloy X meet?
Every Hastelloy X order cites its governing standard (AMS 5536, AMS 5754, ASTM B435, ASTM B572) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Hastelloy X stop being the right choice?
Hastelloy X stops being right above 1100 °C, or in media its family was not built for.