Applications
Hot, pressurized or corrosive duty, usually all three. These six industries run RAS Thermal alloys where ordinary steels stop working.
Market Segments
§01, 01 - 06
Aerospace
Turbine discs, engine rings and fastener stock in 718, Waspaloy and A-286. 718 holds 1275 MPa tensile after solution plus age, and every delivery ships to AMS specification with heat traceability.
718 / Waspaloy / A-286

Oil & Gas
Sour service is a hardness problem as much as a chemistry one. Downhole tools, completion springs and subsea fittings in 625, 825 and K-500 all ship inside ANSI/NACE MR0175 limits for H₂S duty.
625 / 825 / K-500

Petrochemical
C-276 and C22 put PREN at 55 or better, which is what aggressive acid and chloride media demand. Reactor internals, flanges and piping get picked on pitting and stress-corrosion resistance, and 800H covers the hot reformer tubes.
C-276 / C-22 / 800H

Nuclear Power
690 tubing with 30% chromium resists primary-water SCC where 600 cracked. Steam generator tube, core springs and structural fasteners ship with grain size, UT and PMI reporting attached to the PO.
690 / 600 / X-750

Medical
MP35N stays non-magnetic after severe cold work, which implants and guidewires care about. Cobalt-based wire and bar for orthopedic implants, guidewires and surgical instruments, with cleanroom-compatible packaging available.
MP35N / L605 / 35NLT

Marine
Monel 400 for flowing seawater, K-500 aged to 965 MPa tensile for shafting. Propeller shafts, pump components and desalination hardware carry proven seawater and cavitation-erosion resistance.
Monel 400 / K-500