Ask a superalloy supplier certification (en 10204) question about Incoloy 800 (N08800) and the answer lives in the verified reference data Incoloy 800 is built to. This is the practical guide to superalloy supplier certification (en 10204) on Incoloy 800, drawn from RAS Thermal’s superalloy documentation.

Incoloy 800 (N08800) is a Incoloy alloy rated to 1100 °C, stocked for Ethylene furnace tubes.

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Supplier Certification (EN 10204) means for Incoloy 800

For Incoloy 800 (N08800), superalloy supplier certification (en 10204) comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

PropertyIncoloy 800
GradeIncoloy 800 (N08800) · GB NS111
Density7.94 g/cm³
Max service temp1100 °C
Best dutyPetrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASTM B408, ASME SB-407

Specification signals

Ask for 3.1 and the manufacturer attests the heat chemistry for Incoloy 800, ask for 3.2 and a third party stands beside the release. The documented applications tell the same story (ethylene furnace tubes, heat exchanger bundles), and a duty outside that list deserves a second look before Incoloy 800 goes on the order.

  • One Incoloy 800 datasheet callout does most of the work on this page: ASME code approved. A purchasing audit on the Incoloy 800 order checks that line first.

In practice

Generic brochures describe Incoloy 800, while a 3.1 certificate names the actual heat and the actual standard, which is the difference that survives an audit. petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C survives a review because the heat numbers and the OES results can be pulled and re-checked.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy supplier certification (en 10204) resolve for Incoloy 800?

Traceability for Incoloy 800 runs through EN 10204. 3.1 heat chemistry as standard. 3.2 is where a third party must witness. The proof is chemistry. Heat-specific OES results on the certificate, matched to the standard’s band, are what make the grade real.

What is Incoloy 800 best used for?

Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C. The cost-effective Ni-Fe-Cr workhorse for furnace tubes and heat exchangers, oxidation and carburization resistant to 1100 °C.

What forms is Incoloy 800 available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Incoloy 800 meet?

Incoloy 800 ships against ASTM B163, ASTM B407, ASTM B408, ASME SB-407 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Incoloy 800 stop being the right choice?

The ceiling is 1100 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.