Superalloy Supplier Certification (EN 10204), applied to Inconel 718 (N07718): verified numbers first, then the reasoning a specifier applies to Inconel 718. A RAS Thermal reference page on superalloy supplier certification (en 10204).
Inconel 718 (N07718) is a Inconel alloy rated to 650 °C, stocked for Turbine discs and rings.
Inconel 718 (N07718) carries a verified composition band of Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%: the range each element must fall in per the governing standard, and the band the mill certificate cites.
What Superalloy Supplier Certification (EN 10204) means for Inconel 718
Start from the verified triple for Inconel 718: 8.19 g/cm³ density, 650 °C ceiling. On superalloy supplier certification (en 10204) the duty decides, and the duty is rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
| Property | Inconel 718 |
|---|---|
| Grade | Inconel 718 (N07718) |
| Density | 8.19 g/cm³ |
| Max service temp | 650 °C |
| Best duty | Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C |
| Available forms | Forging, Wire, Spring Wire, Bar, Plate, Strip |
| Standards | AMS 5662, AMS 5663, ASTM B637, UNS N07718 |
Specification signals
The grade becomes provable at the moment a heat number and an EN 10204 certificate are issued together for Inconel 718. In practice the applications list confirms the fit: Inconel 718 is specified for turbine discs and rings and compressor blades and fasteners, not as a universal filler.
- One Inconel 718 datasheet callout does most of the work on this page: Precipitation-hardenable to 38 HRC. A purchasing audit on the Inconel 718 order checks that line first.
In practice
Generic brochures describe Inconel 718, while a 3.1 certificate names the actual heat and the actual standard, which is the difference that survives an audit. rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C is only as verifiable as the certificate behind it.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy supplier certification (en 10204) resolve for Inconel 718?
Heat chemistry is the anchor. Witnessed release adds a signature.
What is Inconel 718 best used for?
Inconel 718 is stocked for rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C; the documented edge is that the precipitation-hardened workhorse for turbine discs and fasteners, age-hardened to 38 HRC with usable strength to 650 °C.
What forms is Inconel 718 available in?
The stocked forms are Forging, Wire, Spring Wire, Bar, Plate, Strip; sizes follow the stock range for the form you pick.
What standards does Inconel 718 meet?
Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Inconel 718 stop being the right choice?
The ceiling is 650 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.