What Nimonic 80A (N07080) can and cannot do on superalloy supplier certification (en 10204) is fixed by the verified envelope below. Datasheet facts on Nimonic 80A, and the decision they drive for superalloy supplier certification (en 10204). Nothing else.
Nimonic 80A is a precipitation-hardenable nickel-chromium alloy with additions of titanium and aluminum for gamma-prime strengthening.
For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.
What Superalloy Supplier Certification (EN 10204) means for Nimonic 80A
Nimonic 80A (N07080) on superalloy supplier certification (en 10204): density 8.19 g/cm³, verified ceiling 815 °C. The deciding facts are temperature, media and form, and they land on exhaust valves, turbine blades and high-temperature springs to 815 °C.
| Property | Nimonic 80A |
|---|---|
| Grade | Nimonic 80A (N07080) · GB GH4080A |
| Density | 8.19 g/cm³ |
| Max service temp | 815 °C |
| Best duty | Exhaust valves, turbine blades and high-temperature springs to 815 °C |
| Available forms | Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet |
| Standards | ASTM B637, BS HR 201, AMS 5763, DIN 17742 |
Specification signals
Nimonic 80A is proven on paper by EN 10204, with 3.1 carrying the heat’s own chemistry and 3.2 adding an independent witness. In practice the applications list confirms the fit: Nimonic 80A is specified for automotive exhaust valves and marine diesel engine valves, not as a universal filler.
- The feature that separates Nimonic 80A from its nearest neighbours is specific: Gamma-prime strengthened. Hold the Nimonic 80A certificate to proving it, not asserting it.
In practice
Against ASTM B637 / BS HR 201 (GB GH4080A), the certificate proves the grade by OES chemistry, not a generic datasheet. Once the certificate names the heat, the chemistry and the standard, exhaust valves, turbine blades and high-temperature springs to 815 °C carries proof instead of promises.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy supplier certification (en 10204) resolve for Nimonic 80A?
Nimonic 80A is proven on paper by EN 10204, with 3.1 carrying the heat’s own chemistry and 3.2 adding an independent witness. Generic brochures describe Nimonic 80A, while a 3.1 certificate names the actual heat and the actual standard, which is the difference that survives an audit.
What is Nimonic 80A best used for?
Exhaust valves, turbine blades and high-temperature springs to 815 °C, which is where this grade’s datasheet numbers are actually verified.
What forms is Nimonic 80A available in?
The stocked forms are Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet; sizes follow the stock range for the form you pick.
What standards does Nimonic 80A meet?
Every Nimonic 80A order cites its governing standard (ASTM B637, BS HR 201, AMS 5763, DIN 17742) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Nimonic 80A stop being the right choice?
Nimonic 80A stops being right above 815 °C, or in media its family was not built for.