Waspaloy (N07001) is a Waspaloy grade whose datasheet leans on one documented property: Exceptional creep-rupture strength to 870°C.
As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.
What Superalloy Supplier Certification (EN 10204) means for Waspaloy
Start from the verified triple for Waspaloy: 8.22 g/cm³ density, 870 °C ceiling. On superalloy supplier certification (en 10204) the duty decides, and the duty is turbine discs, rings, shafts and high-temperature fasteners.
| Property | Waspaloy |
|---|---|
| Grade | Waspaloy (N07001) · GB GH4738 |
| Density | 8.22 g/cm³ |
| Max service temp | 870 °C |
| Best duty | Turbine discs, rings, shafts and high-temperature fasteners |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip |
| Standards | AMS 5708, AMS 5709, AMS 5544, ASTM B637 |
Specification signals
Waspaloy is proven on paper by EN 10204, with 3.1 carrying the heat’s own chemistry and 3.2 adding an independent witness. The documented applications tell the same story (turbine discs and rings, compressor shafts), and a duty outside that list deserves a second look before Waspaloy goes on the order.
- One Waspaloy datasheet callout does most of the work on this page: Aerospace turbine grade qualified. A purchasing audit on the Waspaloy order checks that line first.
In practice
A certificate that cannot name the heat and the standard is a brochure. 3.1 exists precisely to close that gap. Provable from heat to part.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy supplier certification (en 10204) resolve for Waspaloy?
For Waspaloy, traceability is the EN 10204 certificate: 3.1 with heat-specific chemistry from the manufacturer, or 3.2 with third-party witnessing. OES makes the grade real.
What is Waspaloy best used for?
Turbine discs, rings, shafts and high-temperature fasteners. A Ni-Cr-Co age-hardenable grade with creep-rupture strength across 650 to 870 °C.
What forms is Waspaloy available in?
Waspaloy ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, within the stock range of each form.
What standards does Waspaloy meet?
AMS 5708, AMS 5709, AMS 5544, ASTM B637 are the standards Waspaloy is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Waspaloy stop being the right choice?
Two things end it: a peak service temperature above 870 °C, or media outside the family Waspaloy was built for.