What Hastelloy C-276 (N10276) can and cannot do on superalloy cold and hot working is fixed by the verified envelope below. Datasheet facts on Hastelloy C-276, and the decision they drive for superalloy cold and hot working. Nothing else.

Hastelloy C-276 (N10276): Versatile nickel-molybdenum-chromium alloy for extreme corrosion resistance..

Hastelloy C-276 (N10276) is bought to a composition band of Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5%; both the governing standard and the mill certificate are read against it.

What Superalloy Cold and Hot Working means for Hastelloy C-276

Hastelloy C-276 (N10276) on superalloy cold and hot working: density 8.89 g/cm³, verified ceiling 400 °C. The deciding facts are temperature, media and form, and they land on chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.

PropertyHastelloy C-276
GradeHastelloy C-276 (N10276)
Density8.89 g/cm³
Max service temp400 °C
Best dutyChemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy
Available formsForging, Wire, Plate, Sheet, Strip, Bar, Tube
StandardsASTM B575, ASTM B574, ASTM B564, UNS N10276

Specification signals

The route for Hastelloy C-276 is never generic, because Forging, Wire, Plate, Sheet, Strip, Bar, Tube do not all survive the same working temperature. In practice the applications list confirms the fit: Hastelloy C-276 is specified for chemical reactor internals and flue-gas desulfurization scrubbers, not as a universal filler.

  • The feature that separates Hastelloy C-276 from its nearest neighbours is specific: Wide acid resistance range. Hold the Hastelloy C-276 certificate to proving it, not asserting it.

In practice

Only the certified end state counts. When the certificate confirms the route’s end state, chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy is traceable from the first heat to the final form.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy cold and hot working resolve for Hastelloy C-276?

For Hastelloy C-276, cold working (wire drawing, strip rolling) and hot working (ring rolling, open-die forging) follow the form: Forging, Wire, Plate, Sheet, Strip, Bar, Tube. Skip the required anneal and the certificate cannot honestly state the condition the drawing called for.

What is Hastelloy C-276 best used for?

Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy. The general-purpose Ni-Cr-Mo corrosion grade for aggressive wet service, weldable without post-weld heat treatment.

What forms is Hastelloy C-276 available in?

Hastelloy C-276 ships as Forging, Wire, Plate, Sheet, Strip, Bar, Tube, within the stock range of each form.

What standards does Hastelloy C-276 meet?

ASTM B575, ASTM B574, ASTM B564, UNS N10276 are the standards Hastelloy C-276 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.

When does Hastelloy C-276 stop being the right choice?

The ceiling is 400 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.