What Incoloy 800HT (N08811) can and cannot do on superalloy cold and hot working is fixed by the verified envelope below. Datasheet facts on Incoloy 800HT, and the decision they drive for superalloy cold and hot working. Nothing else.
Incoloy 800HT (N08811): Fine-grain variant of 800H with optimized high-temperature ductility for forming operations..
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What Superalloy Cold and Hot Working means for Incoloy 800HT
Incoloy 800HT (N08811) on superalloy cold and hot working: density 7.94 g/cm³, verified ceiling 1100 °C. The deciding facts are temperature, media and form, and they land on hot-formed pressure vessel heads, tube sheets and reformer tubes.
| Property | Incoloy 800HT |
|---|---|
| Grade | Incoloy 800HT (N08811) |
| Density | 7.94 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | Hot-formed pressure vessel heads, tube sheets and reformer tubes |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B163, ASTM B407, ASME SB-163, NACE MR0175 |
Specification signals
Incoloy 800HT answers the hot or cold question before the hammer is ordered, through Optimized for hot forming. The documented applications tell the same story (hot-formed pressure vessel heads, heat exchanger tube sheets), and a duty outside that list deserves a second look before Incoloy 800HT goes on the order.
- The feature that separates Incoloy 800HT from its nearest neighbours is specific: Retains 800 family corrosion resistance. Hold the Incoloy 800HT certificate to proving it, not asserting it.
In practice
Forged, drawn or rolled, the part is only releasable once its final condition is the one the purchase order demanded. That is the working window hot-formed pressure vessel heads, tube sheets and reformer tubes is executed in.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy cold and hot working resolve for Incoloy 800HT?
Incoloy 800HT: Optimized for hot forming. Forged, drawn or rolled, the part is only releasable once its final condition is the one the purchase order demanded.
What is Incoloy 800HT best used for?
Hot-formed pressure vessel heads, tube sheets and reformer tubes. The fine-grain 800H variant optimized for hot forming with the 800 family’s high-temperature strength and corrosion resistance.
What forms is Incoloy 800HT available in?
The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.
What standards does Incoloy 800HT meet?
Incoloy 800HT ships against ASTM B163, ASTM B407, ASME SB-163, NACE MR0175 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Incoloy 800HT stop being the right choice?
Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800HT was built for.