Ask a nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) question about Hastelloy C-276 (N10276) and the answer lives in the verified reference data Hastelloy C-276 is built to. This is the specification guide to nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) on Hastelloy C-276, drawn from RAS Thermal’s superalloy documentation.

Hastelloy C-276 is a nickel-molybdenum-chromium alloy for aggressive wet-corrosion service.

Hastelloy C-276 (N10276) is bought to a composition band of Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5%; both the governing standard and the mill certificate are read against it.

What Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo) means for Hastelloy C-276

Hastelloy C-276 (N10276) on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo): density 8.89 g/cm³, verified ceiling 400 °C. The deciding facts are temperature, media and form, and they land on chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.

PropertyHastelloy C-276
GradeHastelloy C-276 (N10276)
Density8.89 g/cm³
Max service temp400 °C
Best dutyChemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy
Available formsForging, Wire, Plate, Sheet, Strip, Bar, Tube
StandardsASTM B575, ASTM B574, ASTM B564, UNS N10276

Specification signals

Family first: Hastelloy C-276 belongs to the nickel line, Ni-Cr / Ni-Fe-Cr / Ni-Cu, Hastelloy series. The documented applications tell the same story (chemical reactor internals, flue-gas desulfurization scrubbers), and a duty outside that list deserves a second look before Hastelloy C-276 goes on the order.

  • One Hastelloy C-276 datasheet callout does most of the work on this page: Good weldability without post-weld heat treatment. A purchasing audit on the Hastelloy C-276 order checks that line first.

In practice

Crevice geometry and peak temperature finish the job that family membership only starts. Once the media fits the family envelope, Hastelloy C-276 for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy is a justified pick rather than a habit.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) resolve for Hastelloy C-276?

Family first: Hastelloy C-276 belongs to the nickel line, Ni-Cr / Ni-Fe-Cr / Ni-Cu, Hastelloy series. Inside the Hastelloy series the alloying balance already hints which media Hastelloy C-276 accepts and which it refuses.

What is Hastelloy C-276 best used for?

Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy, which is where this grade’s datasheet numbers are actually verified.

What forms is Hastelloy C-276 available in?

Hastelloy C-276 ships as Forging, Wire, Plate, Sheet, Strip, Bar, Tube, within the stock range of each form.

What standards does Hastelloy C-276 meet?

Hastelloy C-276 ships against ASTM B575, ASTM B574, ASTM B564, UNS N10276 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Hastelloy C-276 stop being the right choice?

The ceiling is 400 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.