Ask a nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) question about Incoloy 800 (N08800) and the answer lives in the verified reference data Incoloy 800 is built to. This is the specification guide to nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) on Incoloy 800, drawn from RAS Thermal’s superalloy documentation.

Incoloy 800 is an iron-nickel-chromium alloy with good strength and oxidation/carburization resistance at high temperatures.

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo) means for Incoloy 800

For Incoloy 800 (N08800), nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

PropertyIncoloy 800
GradeIncoloy 800 (N08800) · GB NS111
Density7.94 g/cm³
Max service temp1100 °C
Best dutyPetrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASTM B408, ASME SB-407

Specification signals

The nickel line is where Incoloy 800 draws its corrosion character from, with the Incoloy series deciding the details. In practice the applications list confirms the fit: Incoloy 800 is specified for ethylene furnace tubes and heat exchanger bundles, not as a universal filler.

  • The feature that separates Incoloy 800 from its nearest neighbours is specific: Good oxidation resistance to 1100°C. Hold the Incoloy 800 certificate to proving it, not asserting it.

In practice

The Incoloy series works the Ni-Fe-Cr band: high iron content for economy, chromium for oxidation resistance, with molybdenum and copper added where acid duty demands it. petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C is the duty this family position earns.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) resolve for Incoloy 800?

The nickel line is where Incoloy 800 draws its corrosion character from, with the Incoloy series deciding the details. Crevice geometry and peak temperature finish the job that family membership only starts.

What is Incoloy 800 best used for?

Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Incoloy 800 available in?

Incoloy 800 ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.

What standards does Incoloy 800 meet?

Incoloy 800 ships against ASTM B163, ASTM B407, ASTM B408, ASME SB-407 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Incoloy 800 stop being the right choice?

Incoloy 800 stops being right above 1100 °C, or in media its family was not built for.