Most buyers arriving with a nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) question about Incoloy 800H (N08810) need one decision on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo), not a survey. The verified Incoloy 800H data and the routing logic here close it for good.
Incoloy 800H (N08810) is a Incoloy grade whose datasheet leans on one documented property: Enhanced creep strength vs 800.
As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.
What Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo) means for Incoloy 800H
Start from the verified triple for Incoloy 800H: 7.94 g/cm³ density, 1100 °C ceiling. On nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) the duty decides, and the duty is ASME pressure vessels, steam methane reformers and power plant superheaters.
| Property | Incoloy 800H |
|---|---|
| Grade | Incoloy 800H (N08810) · GB NS1102 |
| Density | 7.94 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | ASME pressure vessels, steam methane reformers and power plant superheaters |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII |
Specification signals
Calling Incoloy 800H a nickel alloy says its corrosion answers come out of Ni-Cr / Ni-Fe-Cr / Ni-Cu chemistry, sharpened by the Incoloy series. The documented applications tell the same story (asme pressure vessels, high-temperature heat exchangers), and a duty outside that list deserves a second look before Incoloy 800H goes on the order.
- The feature that separates Incoloy 800H from its nearest neighbours is specific: ASME nuclear/pressure vessel qualified. Hold the Incoloy 800H certificate to proving it, not asserting it.
In practice
Crevice geometry and peak temperature finish the job that family membership only starts. Walk the media and temperature through the nickel filter and ASME pressure vessels, steam methane reformers and power plant superheaters is where Incoloy 800H comes out.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) resolve for Incoloy 800H?
Family first: Incoloy 800H belongs to the nickel line, Ni-Cr / Ni-Fe-Cr / Ni-Cu, Incoloy series. Crevice geometry and peak temperature finish the job that family membership only starts.
What is Incoloy 800H best used for?
ASME pressure vessels, steam methane reformers and power plant superheaters. The controlled-carbon 800 variant with enhanced creep strength for ASME pressure vessel duty above 600 °C.
What forms is Incoloy 800H available in?
Incoloy 800H ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.
What standards does Incoloy 800H meet?
Incoloy 800H ships against ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Incoloy 800H stop being the right choice?
Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800H was built for.