Most buyers arriving with a nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) question about Inconel 718 (N07718) need one decision on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo), not a survey. The verified Inconel 718 data and the routing logic here close it for good.

Inconel 718 is a precipitation-hardenable nickel-chromium alloy with outstanding strength, corrosion resistance and fabricability.

The verified composition band for Inconel 718 (N07718) is Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%; that band is what the mill certificate is checked against, element by element.

What Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo) means for Inconel 718

Inconel 718 (N07718) on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo): density 8.19 g/cm³, verified ceiling 650 °C. The deciding facts are temperature, media and form, and they land on rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.

PropertyInconel 718
GradeInconel 718 (N07718)
Density8.19 g/cm³
Max service temp650 °C
Best dutyRotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C
Available formsForging, Wire, Spring Wire, Bar, Plate, Strip
StandardsAMS 5662, AMS 5663, ASTM B637, UNS N07718

Specification signals

The nickel line is where Inconel 718 draws its corrosion character from, with the Inconel series deciding the details. The documented applications tell the same story (turbine discs and rings, compressor blades and fasteners), and a duty outside that list deserves a second look before Inconel 718 goes on the order.

  • One Inconel 718 datasheet callout does most of the work on this page: Precipitation-hardenable to 38 HRC. A purchasing audit on the Inconel 718 order checks that line first.

In practice

Crevice geometry and peak temperature finish the job that family membership only starts. Once the media fits the family envelope, Inconel 718 for rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C is a justified pick rather than a habit.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) resolve for Inconel 718?

Chemistry family, then grade. Media narrows it next.

What is Inconel 718 best used for?

Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Inconel 718 available in?

Stocked forms: Forging, Wire, Spring Wire, Bar, Plate, Strip.

What standards does Inconel 718 meet?

Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Inconel 718 stop being the right choice?

Inconel 718 stops being right above 650 °C, or in media its family was not built for.