Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo), applied to Nickel 200 (N02200): verified numbers first, then the reasoning a specifier applies to Nickel 200. A RAS Thermal reference page on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo).
Nickel 200 (N02200): Commercially pure wrought nickel for caustic soda, synthetic fiber and electrical applications..
As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.
What Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo) means for Nickel 200
Nickel 200 (N02200) on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo): density 8.89 g/cm³, verified ceiling 315 °C. The deciding facts are temperature, media and form, and they land on caustic soda evaporator tubes, spinnerets and electrical terminals.
| Property | Nickel 200 |
|---|---|
| Grade | Nickel 200 (N02200) · GB N6 |
| Density | 8.89 g/cm³ |
| Max service temp | 315 °C |
| Best duty | Caustic soda evaporator tubes, spinnerets and electrical terminals |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B160, ASTM B161, ASTM B162, ASME SB-160 |
Specification signals
Start with the family label for Nickel 200, Ni-Cr / Ni-Fe-Cr / Ni-Cu inside the Pure Nickel series, and the media routing already narrows. The documented applications tell the same story (caustic soda evaporator tubes, synthetic fiber spinnerets), and a duty outside that list deserves a second look before Nickel 200 goes on the order.
- The feature that separates Nickel 200 from its nearest neighbours is specific: Food-grade qualified. Hold the Nickel 200 certificate to proving it, not asserting it.
In practice
The grade-specific claim: Excellent caustic alkali resistance. caustic soda evaporator tubes, spinnerets and electrical terminals is the duty this family position earns.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) resolve for Nickel 200?
Nickel 200 sits in the nickel family (Ni-Cr / Ni-Fe-Cr / Ni-Cu), in the Pure Nickel series. Inside the Pure Nickel series the alloying balance already hints which media Nickel 200 accepts and which it refuses.
What is Nickel 200 best used for?
Caustic soda evaporator tubes, spinnerets and electrical terminals, which is where this grade’s datasheet numbers are actually verified.
What forms is Nickel 200 available in?
Nickel 200 ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.
What standards does Nickel 200 meet?
ASTM B160, ASTM B161, ASTM B162, ASME SB-160 are the standards Nickel 200 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Nickel 200 stop being the right choice?
Two things end it: a peak service temperature above 315 °C, or media outside the family Nickel 200 was built for.