What Nimonic 80A (N07080) can and cannot do on nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) is fixed by the verified envelope below. Datasheet facts on Nimonic 80A, and the decision they drive for nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo). Nothing else.
Nimonic 80A (N07080) is a Nimonic grade whose datasheet leans on one documented property: Precipitation-hardenable.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What Nickel Alloy Corrosion Families (Ni-Cr-Mo, Ni-Cu, Ni-Mo) means for Nimonic 80A
What fixes nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) for Nimonic 80A (N07080) is the verified envelope (8.19 g/cm³, 815 °C) read against exhaust valves, turbine blades and high-temperature springs to 815 °C.
| Property | Nimonic 80A |
|---|---|
| Grade | Nimonic 80A (N07080) · GB GH4080A |
| Density | 8.19 g/cm³ |
| Max service temp | 815 °C |
| Best duty | Exhaust valves, turbine blades and high-temperature springs to 815 °C |
| Available forms | Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet |
| Standards | ASTM B637, BS HR 201, AMS 5763, DIN 17742 |
Specification signals
Calling Nimonic 80A a nickel alloy says its corrosion answers come out of Ni-Cr / Ni-Fe-Cr / Ni-Cu chemistry, sharpened by the Nimonic series. In practice the applications list confirms the fit: Nimonic 80A is specified for automotive exhaust valves and marine diesel engine valves, not as a universal filler.
- The feature that separates Nimonic 80A from its nearest neighbours is specific: Exhaust valve industry standard. Hold the Nimonic 80A certificate to proving it, not asserting it.
In practice
Inside the Nimonic series the alloying balance already hints which media Nimonic 80A accepts and which it refuses. Which is why exhaust valves, turbine blades and high-temperature springs to 815 °C lands on this grade.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does nickel alloy corrosion families (ni-cr-mo, ni-cu, ni-mo) resolve for Nimonic 80A?
Nimonic 80A sits in the nickel family (Ni-Cr / Ni-Fe-Cr / Ni-Cu), in the Nimonic series. Family routing is the first filter, not the last word. Media, temperature and crevice geometry narrow it to a grade.
What is Nimonic 80A best used for?
Exhaust valves, turbine blades and high-temperature springs to 815 °C, which is where this grade’s datasheet numbers are actually verified.
What forms is Nimonic 80A available in?
The stocked forms are Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet; sizes follow the stock range for the form you pick.
What standards does Nimonic 80A meet?
Nimonic 80A ships against ASTM B637, BS HR 201, AMS 5763, DIN 17742 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Nimonic 80A stop being the right choice?
Nimonic 80A stops being right above 815 °C, or in media its family was not built for.