What 1J50 can and cannot do on superalloy density and weight is fixed by the verified envelope below. Datasheet facts on 1J50, and the decision they drive for superalloy density and weight. Nothing else.

1J50: Soft magnetic Fe-Ni alloy with high permeability and low coercivity for transformer cores and magnetic shielding..

For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.

What Superalloy Density and Weight means for 1J50

Start from the verified triple for 1J50: 8.2 g/cm³ density, 450 °C ceiling. On superalloy density and weight the duty decides, and the duty is instrument transformer cores, relay armatures and shielding.

Property1J50
Grade1J50
Density8.2 g/cm³
Max service temp450 °C
Best dutyInstrument transformer cores, relay armatures and shielding
Available formsWire, Strip, Plate & Sheet, Bar & Rod
StandardsGB/T 14986, IEC 60404-8-6

Specification signals

The mass conversation for 1J50 opens and closes with 8.2 g/cm³. In practice the applications list confirms the fit: 1J50 is specified for instrument transformer cores and magnetic amplifier laminations, not as a universal filler.

  • One 1J50 datasheet callout does most of the work on this page: High saturation induction. A purchasing audit on the 1J50 order checks that line first.

In practice

Volume is fixed by the drawing, so density is the only lever 1J50 leaves the weight engineer. Budget the mass honestly.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy density and weight resolve for 1J50?

Start every mass estimate for 1J50 from 8.2 g/cm³, the one figure the calculation cannot dodge. Weight per part = density × volume, so this is the figure every bar, plate or forging mass estimate starts from.

What is 1J50 best used for?

Instrument transformer cores, relay armatures and shielding, which is where this grade’s datasheet numbers are actually verified.

What forms is 1J50 available in?

1J50 ships as Wire, Strip, Plate & Sheet, Bar & Rod, within the stock range of each form.

What standards does 1J50 meet?

Every 1J50 order cites its governing standard (GB/T 14986, IEC 60404-8-6) and arrives with an EN 10204 3.1 certificate proving the heat.

When does 1J50 stop being the right choice?

The ceiling is 450 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.