Ask a superalloy density and weight question about Incoloy 800H (N08810) and the answer lives in the verified reference data Incoloy 800H is built to. This is the specification guide to superalloy density and weight on Incoloy 800H, drawn from RAS Thermal’s superalloy documentation.

Incoloy 800H is an alloy supplied against its verified datasheet and the governing standard.

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Density and Weight means for Incoloy 800H

For Incoloy 800H (N08810), superalloy density and weight comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as ASME pressure vessels, steam methane reformers and power plant superheaters.

PropertyIncoloy 800H
GradeIncoloy 800H (N08810) · GB NS1102
Density7.94 g/cm³
Max service temp1100 °C
Best dutyASME pressure vessels, steam methane reformers and power plant superheaters
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII

Specification signals

Density does the arithmetic quietly, and for Incoloy 800H the arithmetic begins at 7.94 g/cm³. In practice the applications list confirms the fit: Incoloy 800H is specified for asme pressure vessels and high-temperature heat exchangers, not as a universal filler.

  • The feature that separates Incoloy 800H from its nearest neighbours is specific: Controlled carbon for carburization resistance. Hold the Incoloy 800H certificate to proving it, not asserting it.

In practice

Weight per part = density × volume, so this is the figure every bar, plate or forging mass estimate starts from. Carry 7.94 g/cm³ into the budget and ASME pressure vessels, steam methane reformers and power plant superheaters gets weighed before it is ordered.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy density and weight resolve for Incoloy 800H?

One verified figure, 7.94 g/cm³, sits beneath the whole weight discussion for Incoloy 800H. On weight-budgeted hardware the density is a design input, not trivia. It scales every volume-based cost line.

What is Incoloy 800H best used for?

Incoloy 800H is stocked for ASME pressure vessels, steam methane reformers and power plant superheaters; the documented edge is that the controlled-carbon 800 variant with enhanced creep strength for ASME pressure vessel duty above 600 °C.

What forms is Incoloy 800H available in?

Incoloy 800H ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.

What standards does Incoloy 800H meet?

Every Incoloy 800H order cites its governing standard (ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Incoloy 800H stop being the right choice?

Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800H was built for.