What Incoloy 800HT (N08811) can and cannot do on superalloy density and weight is fixed by the verified envelope below. Datasheet facts on Incoloy 800HT, and the decision they drive for superalloy density and weight. Nothing else.
Incoloy 800HT (N08811): Fine-grain variant of 800H with optimized high-temperature ductility for forming operations..
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What Superalloy Density and Weight means for Incoloy 800HT
Incoloy 800HT (N08811) on superalloy density and weight: density 7.94 g/cm³, verified ceiling 1100 °C. The deciding facts are temperature, media and form, and they land on hot-formed pressure vessel heads, tube sheets and reformer tubes.
| Property | Incoloy 800HT |
|---|---|
| Grade | Incoloy 800HT (N08811) |
| Density | 7.94 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | Hot-formed pressure vessel heads, tube sheets and reformer tubes |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B163, ASTM B407, ASME SB-163, NACE MR0175 |
Specification signals
The mass conversation for Incoloy 800HT opens and closes with 7.94 g/cm³. The documented applications tell the same story (hot-formed pressure vessel heads, heat exchanger tube sheets), and a duty outside that list deserves a second look before Incoloy 800HT goes on the order.
- One Incoloy 800HT datasheet callout does most of the work on this page: Optimized for hot forming. A purchasing audit on the Incoloy 800HT order checks that line first.
In practice
Every kilogram on the cost line traces back to this multiplication. Mass budgets for hot-formed pressure vessel heads, tube sheets and reformer tubes start here.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy density and weight resolve for Incoloy 800HT?
Start every mass estimate for Incoloy 800HT from 7.94 g/cm³, the one figure the calculation cannot dodge. A wrong density assumption quietly corrupts the quote, the freight and the lifting plan at once.
What is Incoloy 800HT best used for?
Incoloy 800HT is stocked for hot-formed pressure vessel heads, tube sheets and reformer tubes; the documented edge is that the fine-grain 800H variant optimized for hot forming with the 800 family’s high-temperature strength and corrosion resistance.
What forms is Incoloy 800HT available in?
The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.
What standards does Incoloy 800HT meet?
Incoloy 800HT ships against ASTM B163, ASTM B407, ASME SB-163, NACE MR0175 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Incoloy 800HT stop being the right choice?
Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800HT was built for.