Ask a superalloy density and weight question about Inconel 625 (N06625) and the answer lives in the verified reference data Inconel 625 is built to. This is the specification guide to superalloy density and weight on Inconel 625, drawn from RAS Thermal’s superalloy documentation.
Inconel 625 (N06625) is a Inconel grade whose datasheet leans on one documented property: Excellent pitting and crevice corrosion resistance.
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What Superalloy Density and Weight means for Inconel 625
For Inconel 625 (N06625), superalloy density and weight comes down to the documented envelope: 8.44 g/cm³, 980 °C ceiling, and a duty best described as seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide.
| Property | Inconel 625 |
|---|---|
| Grade | Inconel 625 (N06625) · GB GH3625 |
| Density | 8.44 g/cm³ |
| Max service temp | 980 °C |
| Best duty | Seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide |
| Available forms | Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube |
| Standards | ASTM B443, ASTM B444, ASTM B446, AMS 5666, NACE MR0175 |
Specification signals
Inconel 625 verifies at 8.44 g/cm³, and that is the number to carry into any mass calculation. The documented applications tell the same story (seawater piping and risers, chemical processing equipment), and a duty outside that list deserves a second look before Inconel 625 goes on the order.
- One Inconel 625 datasheet callout does most of the work on this page: Excellent weldability. A purchasing audit on the Inconel 625 order checks that line first.
In practice
Every kilogram on the cost line traces back to this multiplication. seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide inherits that number directly.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy density and weight resolve for Inconel 625?
Density, verified for Inconel 625: 8.44 g/cm³. Mass estimates are honest exactly when they start from the verified figure, 8.44 g/cm³, instead of a family average.
What is Inconel 625 best used for?
Seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide. A solid-solution Ni-Cr-Mo alloy that keeps both strength and corrosion resistance from cryogenic to 980 °C.
What forms is Inconel 625 available in?
Inconel 625 ships as Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube, within the stock range of each form.
What standards does Inconel 625 meet?
ASTM B443, ASTM B444, ASTM B446, AMS 5666, NACE MR0175 are the standards Inconel 625 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Inconel 625 stop being the right choice?
Inconel 625 stops being right above 980 °C, or in media its family was not built for.