Ask a superalloy density and weight question about Nimonic 80A (N07080) and the answer lives in the verified reference data Nimonic 80A is built to. This is the specification guide to superalloy density and weight on Nimonic 80A, drawn from RAS Thermal’s superalloy documentation.
Nimonic 80A (N07080) is a Nimonic alloy rated to 815 °C, stocked for Automotive exhaust valves.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What Superalloy Density and Weight means for Nimonic 80A
Nimonic 80A (N07080) on superalloy density and weight: density 8.19 g/cm³, verified ceiling 815 °C. The deciding facts are temperature, media and form, and they land on exhaust valves, turbine blades and high-temperature springs to 815 °C.
| Property | Nimonic 80A |
|---|---|
| Grade | Nimonic 80A (N07080) · GB GH4080A |
| Density | 8.19 g/cm³ |
| Max service temp | 815 °C |
| Best duty | Exhaust valves, turbine blades and high-temperature springs to 815 °C |
| Available forms | Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet |
| Standards | ASTM B637, BS HR 201, AMS 5763, DIN 17742 |
Specification signals
Verified once, multiplied everywhere. In practice the applications list confirms the fit: Nimonic 80A is specified for automotive exhaust valves and marine diesel engine valves, not as a universal filler.
- The feature that separates Nimonic 80A from its nearest neighbours is specific: 815°C service temperature. Hold the Nimonic 80A certificate to proving it, not asserting it.
In practice
Volume is fixed by the drawing, so density is the only lever Nimonic 80A leaves the weight engineer. Freight, forging and handling costs for exhaust valves, turbine blades and high-temperature springs to 815 °C all scale from the same 8.19 g/cm³ starting point.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy density and weight resolve for Nimonic 80A?
Nimonic 80A verifies at 8.19 g/cm³, and that is the number to carry into any mass calculation. Multiply 8.19 g/cm³ by the section volume and the quote’s mass line stops being a surprise.
What is Nimonic 80A best used for?
Exhaust valves, turbine blades and high-temperature springs to 815 °C, which is where this grade’s datasheet numbers are actually verified.
What forms is Nimonic 80A available in?
Stocked forms: Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet.
What standards does Nimonic 80A meet?
Nimonic 80A ships against ASTM B637, BS HR 201, AMS 5763, DIN 17742 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Nimonic 80A stop being the right choice?
The ceiling is 815 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.