Most buyers arriving with a superalloy density and weight question about Waspaloy (N07001) need one decision on superalloy density and weight, not a survey. The verified Waspaloy data and the routing logic here close it for good.

Waspaloy (N07001) is a Waspaloy grade whose datasheet leans on one documented property: Exceptional creep-rupture strength to 870°C.

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What Superalloy Density and Weight means for Waspaloy

For Waspaloy (N07001), superalloy density and weight comes down to the documented envelope: 8.22 g/cm³, 870 °C ceiling, and a duty best described as turbine discs, rings, shafts and high-temperature fasteners.

PropertyWaspaloy
GradeWaspaloy (N07001) · GB GH4738
Density8.22 g/cm³
Max service temp870 °C
Best dutyTurbine discs, rings, shafts and high-temperature fasteners
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip
StandardsAMS 5708, AMS 5709, AMS 5544, ASTM B637

Specification signals

Verified once, multiplied everywhere. The documented applications tell the same story (turbine discs and rings, compressor shafts), and a duty outside that list deserves a second look before Waspaloy goes on the order.

  • The feature that separates Waspaloy from its nearest neighbours is specific: Precipitation-hardenable for turbine applications. Hold the Waspaloy certificate to proving it, not asserting it.

In practice

Mass estimates are honest exactly when they start from the verified figure, 8.22 g/cm³, instead of a family average. turbine discs, rings, shafts and high-temperature fasteners inherits that number directly.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy density and weight resolve for Waspaloy?

Waspaloy verifies at 8.22 g/cm³, and that is the number to carry into any mass calculation. Mass estimates are honest exactly when they start from the verified figure, 8.22 g/cm³, instead of a family average.

What is Waspaloy best used for?

Waspaloy is stocked for turbine discs, rings, shafts and high-temperature fasteners; the documented edge is that a Ni-Cr-Co age-hardenable grade with creep-rupture strength across 650 to 870 °C.

What forms is Waspaloy available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip; sizes follow the stock range for the form you pick.

What standards does Waspaloy meet?

Waspaloy ships against AMS 5708, AMS 5709, AMS 5544, ASTM B637 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Waspaloy stop being the right choice?

The ceiling is 870 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.