Ask a superalloy hardness (hrc / hrb) question about 4J29 and the answer lives in the verified reference data 4J29 is built to. This is the specification guide to superalloy hardness (hrc / hrb) on 4J29, drawn from RAS Thermal’s superalloy documentation.
4J29: Kovar, Fe-Ni-Co expansion alloy for glass-to-metal and ceramic-to-metal seals in electronics packaging..
For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.
What Superalloy Hardness (HRC / HRB) means for 4J29
4J29 on superalloy hardness (hrc / hrb): density 8.17 g/cm³, verified ceiling 450 °C. The deciding facts are temperature, media and form, and they land on glass-to-metal and ceramic-to-metal seals in electronic packages.
| Property | 4J29 |
|---|---|
| Grade | 4J29 |
| Density | 8.17 g/cm³ |
| Max service temp | 450 °C |
| Best duty | Glass-to-metal and ceramic-to-metal seals in electronic packages |
| Available forms | Wire, Strip, Bar & Rod, Plate & Sheet |
| Standards | ASTM F15, GB/T 14986, MIL-I-23011 |
Specification signals
No single hardness number is claimed for 4J29. The band is set by the supply condition. The documented applications tell the same story (transistor and ic hermetic packages, microwave tube windows), and a duty outside that list deserves a second look before 4J29 goes on the order.
- The feature that separates 4J29 from its nearest neighbours is specific: Kovar / ASTM F15 standard. Hold the 4J29 certificate to proving it, not asserting it.
In practice
The EN 10204 3.1 certificate is where the actual hardness of your heat appears. glass-to-metal and ceramic-to-metal seals in electronic packages behaves as drawn only when the supplied condition matches the band the designer assumed.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy hardness (hrc / hrb) resolve for 4J29?
4J29 is supplied to the hardness band its condition implies, and the certificate states the value. Confirm the target band on the certificate before comparing grades. Conditions, not alloys, set most hardness differences.
What is 4J29 best used for?
4J29 is stocked for glass-to-metal and ceramic-to-metal seals in electronic packages; the documented edge is that the Kovar expansion alloy whose expansion matches borosilicate glass for hermetic seals.
What forms is 4J29 available in?
Stocked forms: Wire, Strip, Bar & Rod, Plate & Sheet.
What standards does 4J29 meet?
Every 4J29 order cites its governing standard (ASTM F15, GB/T 14986, MIL-I-23011) and arrives with an EN 10204 3.1 certificate proving the heat.
When does 4J29 stop being the right choice?
Two things end it: a peak service temperature above 450 °C, or media outside the family 4J29 was built for.