Ask a superalloy hardness (hrc / hrb) question about 4J36 and the answer lives in the verified reference data 4J36 is built to. This is the specification guide to superalloy hardness (hrc / hrb) on 4J36, drawn from RAS Thermal’s superalloy documentation.
4J36 is a Precision grade whose datasheet leans on one documented property: Near-zero thermal expansion (α ≈ 1.3 × 10⁻⁶/°C).
For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.
What Superalloy Hardness (HRC / HRB) means for 4J36
Start from the verified triple for 4J36: 8.1 g/cm³ density, 230 °C ceiling. On superalloy hardness (hrc / hrb) the duty decides, and the duty is optical benches, LNG tank membranes and cryogenic transfer lines.
| Property | 4J36 |
|---|---|
| Grade | 4J36 |
| Density | 8.1 g/cm³ |
| Max service temp | 230 °C |
| Best duty | Optical benches, LNG tank membranes and cryogenic transfer lines |
| Available forms | Wire, Strip, Bar & Rod, Plate & Sheet |
| Standards | ASTM F1684, GB/T 14986, AFNOR NF A54-301 |
Specification signals
A single hardness figure for 4J36 would hide the treatment, so the verified data refuse to give one. The documented applications tell the same story (precision optical benches and mounts, lng carrier tank membranes), and a duty outside that list deserves a second look before 4J36 goes on the order.
- One 4J36 datasheet callout does most of the work on this page: Invar 36 standard. A purchasing audit on the 4J36 order checks that line first.
In practice
The EN 10204 3.1 certificate is where the actual hardness of your heat appears. The hardness class and optical benches, LNG tank membranes and cryogenic transfer lines go together on the purchase order.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy hardness (hrc / hrb) resolve for 4J36?
4J36 is supplied to the hardness band its condition implies, and the certificate states the value. Conditions beat brand names.
What is 4J36 best used for?
4J36 is stocked for optical benches, LNG tank membranes and cryogenic transfer lines; the documented edge is that the Invar 36 grade with near-zero thermal expansion for dimensional stability.
What forms is 4J36 available in?
The stocked forms are Wire, Strip, Bar & Rod, Plate & Sheet; sizes follow the stock range for the form you pick.
What standards does 4J36 meet?
4J36 ships against ASTM F1684, GB/T 14986, AFNOR NF A54-301 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does 4J36 stop being the right choice?
4J36 stops being right above 230 °C, or in media its family was not built for.