What Hastelloy C-276 (N10276) can and cannot do on superalloy hardness (hrc / hrb) is fixed by the verified envelope below. Datasheet facts on Hastelloy C-276, and the decision they drive for superalloy hardness (hrc / hrb). Nothing else.

Hastelloy C-276 (N10276) is a Hastelloy alloy rated to 400 °C, stocked for Chemical reactor internals.

Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5% is the certified band for Hastelloy C-276 (N10276): every element bounded by the governing standard and proven on the certificate rather than assumed.

What Superalloy Hardness (HRC / HRB) means for Hastelloy C-276

For Hastelloy C-276 (N10276), superalloy hardness (hrc / hrb) comes down to the documented envelope: 8.89 g/cm³, 400 °C ceiling, and a duty best described as chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.

PropertyHastelloy C-276
GradeHastelloy C-276 (N10276)
Density8.89 g/cm³
Max service temp400 °C
Best dutyChemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy
Available formsForging, Wire, Plate, Sheet, Strip, Bar, Tube
StandardsASTM B575, ASTM B574, ASTM B564, UNS N10276

Specification signals

The reading is 90 HRB for Hastelloy C-276, and it describes a specific heat-treated state rather than the alloy in every form. In practice the applications list confirms the fit: Hastelloy C-276 is specified for chemical reactor internals and flue-gas desulfurization scrubbers, not as a universal filler.

  • The feature that separates Hastelloy C-276 from its nearest neighbours is specific: Wide acid resistance range. Hold the Hastelloy C-276 certificate to proving it, not asserting it.

In practice

The certificate states the hardness of your heat. The datasheet value is the class, the certificate is the evidence. The hardness class and chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy go together on the purchase order.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy hardness (hrc / hrb) resolve for Hastelloy C-276?

90 HRB is the figure the indentation test returns, and a purchaser checks that return against the class before the bar leaves inspection. An aged Hastelloy C-276 part and an annealed one indent differently under the same load, so the condition has to be written beside 90 HRB.

What is Hastelloy C-276 best used for?

Hastelloy C-276 is stocked for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy; the documented edge is that the general-purpose Ni-Cr-Mo corrosion grade for aggressive wet service, weldable without post-weld heat treatment.

What forms is Hastelloy C-276 available in?

Hastelloy C-276 ships as Forging, Wire, Plate, Sheet, Strip, Bar, Tube, within the stock range of each form.

What standards does Hastelloy C-276 meet?

ASTM B575, ASTM B574, ASTM B564, UNS N10276 are the standards Hastelloy C-276 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.

When does Hastelloy C-276 stop being the right choice?

Hastelloy C-276 stops being right above 400 °C, or in media its family was not built for.