Most buyers arriving with a superalloy hardness (hrc / hrb) question about Incoloy 800H (N08810) need one decision on superalloy hardness (hrc / hrb), not a survey. The verified Incoloy 800H data and the routing logic here close it for good.

Incoloy 800H is an alloy supplied against its verified datasheet and the governing standard.

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What Superalloy Hardness (HRC / HRB) means for Incoloy 800H

What fixes superalloy hardness (hrc / hrb) for Incoloy 800H (N08810) is the verified envelope (7.94 g/cm³, 1100 °C) read against ASME pressure vessels, steam methane reformers and power plant superheaters.

PropertyIncoloy 800H
GradeIncoloy 800H (N08810) · GB NS1102
Density7.94 g/cm³
Max service temp1100 °C
Best dutyASME pressure vessels, steam methane reformers and power plant superheaters
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII

Specification signals

The mill supplies Incoloy 800H to the band its treatment implies, then writes the measured value on the certificate. In practice the applications list confirms the fit: Incoloy 800H is specified for asme pressure vessels and high-temperature heat exchangers, not as a universal filler.

  • The feature that separates Incoloy 800H from its nearest neighbours is specific: Good structural stability. Hold the Incoloy 800H certificate to proving it, not asserting it.

In practice

The EN 10204 3.1 certificate is where the actual hardness of your heat appears. The hardness class and ASME pressure vessels, steam methane reformers and power plant superheaters go together on the purchase order.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy hardness (hrc / hrb) resolve for Incoloy 800H?

Incoloy 800H is supplied to the hardness band its condition implies, and the certificate states the value. The EN 10204 3.1 certificate is where the actual hardness of your heat appears.

What is Incoloy 800H best used for?

ASME pressure vessels, steam methane reformers and power plant superheaters, which is where this grade’s datasheet numbers are actually verified.

What forms is Incoloy 800H available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Incoloy 800H meet?

Incoloy 800H ships against ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Incoloy 800H stop being the right choice?

Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800H was built for.