Most buyers arriving with a superalloy hardness (hrc / hrb) question about Inconel 718 (N07718) need one decision on superalloy hardness (hrc / hrb), not a survey. The verified Inconel 718 data and the routing logic here close it for good.
Inconel 718 is a precipitation-hardenable nickel-chromium alloy with outstanding strength, corrosion resistance and fabricability.
The verified composition band for Inconel 718 (N07718) is Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%; that band is what the mill certificate is checked against, element by element.
What Superalloy Hardness (HRC / HRB) means for Inconel 718
Start from the verified triple for Inconel 718: 8.19 g/cm³ density, 650 °C ceiling. On superalloy hardness (hrc / hrb) the duty decides, and the duty is rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
| Property | Inconel 718 |
|---|---|
| Grade | Inconel 718 (N07718) |
| Density | 8.19 g/cm³ |
| Max service temp | 650 °C |
| Best duty | Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C |
| Available forms | Forging, Wire, Spring Wire, Bar, Plate, Strip |
| Standards | AMS 5662, AMS 5663, ASTM B637, UNS N07718 |
Specification signals
The reading is 38 HRC for Inconel 718, and it describes a specific heat-treated state rather than the alloy in every form. The documented applications tell the same story (turbine discs and rings, compressor blades and fasteners), and a duty outside that list deserves a second look before Inconel 718 goes on the order.
- One Inconel 718 datasheet callout does most of the work on this page: AMS 5662 / 5663 rotating-quality certified. A purchasing audit on the Inconel 718 order checks that line first.
In practice
Condition first, number second. Annealed, solution-treated and aged states do not share a hardness band. Once the certificate shows the band for the actual heat, rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C carries a hardness claim an auditor can retest.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy hardness (hrc / hrb) resolve for Inconel 718?
Inconel 718 verifies 38 HRC at room temperature inside its 650 °C envelope. Condition first, number second. Annealed, solution-treated and aged states do not share a hardness band.
What is Inconel 718 best used for?
Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C. The precipitation-hardened workhorse for turbine discs and fasteners, age-hardened to 38 HRC with usable strength to 650 °C.
What forms is Inconel 718 available in?
The stocked forms are Forging, Wire, Spring Wire, Bar, Plate, Strip; sizes follow the stock range for the form you pick.
What standards does Inconel 718 meet?
Every Inconel 718 order cites its governing standard (AMS 5662, AMS 5663, ASTM B637, UNS N07718) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Inconel 718 stop being the right choice?
Inconel 718 stops being right above 650 °C, or in media its family was not built for.