What Nimonic 80A (N07080) can and cannot do on superalloy hardness (hrc / hrb) is fixed by the verified envelope below. Datasheet facts on Nimonic 80A, and the decision they drive for superalloy hardness (hrc / hrb). Nothing else.

Nimonic 80A (N07080): Ni-Cr-Ti-Al alloy for exhaust valves, turbine blades and high-temperature springs..

For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.

What Superalloy Hardness (HRC / HRB) means for Nimonic 80A

Nimonic 80A (N07080) on superalloy hardness (hrc / hrb): density 8.19 g/cm³, verified ceiling 815 °C. The deciding facts are temperature, media and form, and they land on exhaust valves, turbine blades and high-temperature springs to 815 °C.

PropertyNimonic 80A
GradeNimonic 80A (N07080) · GB GH4080A
Density8.19 g/cm³
Max service temp815 °C
Best dutyExhaust valves, turbine blades and high-temperature springs to 815 °C
Available formsForging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet
StandardsASTM B637, BS HR 201, AMS 5763, DIN 17742

Specification signals

Hardness for Nimonic 80A starts with that feature text, Good hot hardness, and ends only when a heat-specific reading confirms it. The documented applications tell the same story (automotive exhaust valves, marine diesel engine valves), and a duty outside that list deserves a second look before Nimonic 80A goes on the order.

  • The feature that separates Nimonic 80A from its nearest neighbours is specific: Good hot hardness. Hold the Nimonic 80A certificate to proving it, not asserting it.

In practice

Condition earns the number. That band is part of what exhaust valves, turbine blades and high-temperature springs to 815 °C depends on.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy hardness (hrc / hrb) resolve for Nimonic 80A?

Nimonic 80A’s verified feature set carries the hardness story: Good hot hardness. Write aged, annealed or solution-treated beside the requirement, because hardness follows condition before it follows alloy.

What is Nimonic 80A best used for?

Exhaust valves, turbine blades and high-temperature springs to 815 °C. The classic gamma-prime strengthened valve alloy, serviceable to 815 °C with good hot hardness.

What forms is Nimonic 80A available in?

Nimonic 80A ships as Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, within the stock range of each form.

What standards does Nimonic 80A meet?

Every Nimonic 80A order cites its governing standard (ASTM B637, BS HR 201, AMS 5763, DIN 17742) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Nimonic 80A stop being the right choice?

Two things end it: a peak service temperature above 815 °C, or media outside the family Nimonic 80A was built for.