Hastelloy C-276 plate is quoted two ways: per kilogram of metal and per square metre of product. The two are linked by one exact relationship — one square metre of plate at t mm weighs 8.89 × t kg, using the specification density of 8.89 g/cm³. Everything else on the enquiry follows from that number plus what your supplier charges for the specific gauge.

What this page does not do is print a per-kilogram band. C-276 carries 15-17 % molybdenum and 3.0-4.5 % tungsten, both of which trade on markets that have nothing to do with your vessel schedule, so a figure frozen here would be wrong before the plate shipped. The ordering between gauges and the arithmetic, on the other hand, stay true.

Plate weight, exact, gauge by gauge

ThicknessWeight per m²Cost positionWhat drives the position
3 mm26.67 kg/m²Highest per kgMost rolling passes, flatness control, largest yield share
5 mm44.45 kg/m²HighFinish and flatness still dominate
6 mm53.34 kg/m²HighCommon gauge; availability helps, process still dear
8 mm71.12 kg/m²Upper midConversion spreading over more weight
10 mm88.90 kg/m²MidWorkhorse gauge for vessels and ducting
12 mm106.68 kg/m²MidSame route, more metal
15 mm133.35 kg/m²Lower midCloser to as-rolled
20 mm177.80 kg/m²Lower midFewer finishing steps
25 mm222.25 kg/m²LowHeavy plate, little finish work
30 mm266.70 kg/m²LowHeavy plate
40 mm355.60 kg/m²LowestMinimum conversion per kilogram
50 mm444.50 kg/m²LowestSlab-adjacent; near-as-rolled condition

The weight column is arithmetic and checkable: 8.89 g/cm³ × 1 mm × 1 m² = 8.89 kg. Multiply by the gauge. A 2,000 × 6,000 mm plate at 10 mm is 12 m², therefore 1,066.8 kg — the figure your freight forwarder will also want.

Why the cost per kilogram falls as the plate gets heavier

Three things change as thickness falls, and all three raise cost per kilogram:

  1. Passes. Reaching 3 mm from a slab takes more rolling passes than reaching 30 mm, and each pass consumes mill time and carries a rejection risk.
  2. Flatness and finish. Thin plate distorts more in handling and in heat treatment, so more of the output is straightened, re-rolled or downgraded.
  3. Yield. Trimming and edge conditioning remove a fixed width of material. On a 3 mm sheet that width is a large fraction of the total; on a 50 mm plate it is noise.

None of that is a pricing trick. It is the same reason a thin stainless sheet costs more per kilogram than a heavy one.

What C-276 is, and why the alloy itself is expensive

C-276 is a nickel-molybdenum-chromium alloy with deliberately low carbon and silicon so that weld zones keep their corrosion resistance. The published ranges from ASTM B575:

  • Molybdenum 15.0-17.0 % — the corrosion workhorse against chlorides and reducing acids
  • Tungsten 3.0-4.5 % — added resistance, and the reason PMI verification matters on this grade
  • Chromium 14.5-16.5 % — oxidising resistance, and enough to keep the passive film
  • Iron 4.0-7.0 %, cobalt 2.5 % max — controlled residuals
  • Density 8.89 g/cm³ — among the densest of the wrought nickel alloys, which is why a C-276 plate weighs more than the same size in 625 or 718

Two of those lines — molybdenum and tungsten — are separately traded commodities. That is why the cost of C-276 follows the molybdenum market more closely than the nickel market, and why a quote on this grade needs a shorter validity window than a quote on 718.

Getting from weight to a comparable quote

A plate enquiry that can be priced without a second round of questions states:

  • Thickness and sheet size, and whether the size is ex-mill or cut
  • Quantity in pieces, kilograms or square metres
  • Standard — ASTM B575 for plate, sheet and strip
  • Certificate level — EN 10204 3.1 to the heat, or 3.2 witnessed
  • Test scope — PMI, UT, or any additional NDT
  • Incoterm and destination port

The RFQ spec writer assembles those lines. Two quotes that both state certificate level and test scope can be compared; two that state only a thickness cannot.

Where this fits against the other grades

If the duty is chloride-bearing but the temperature stays moderate, 625 is often the lower-cost answer — it carries 8-10 % molybdenum instead of 15-17 % plus tungsten, and it welds without post-weld heat treatment. The comparison is worked through on the nickel alloy price guide, and the corrosion reasoning on the corrosion family hub.

Frequently Asked Questions (FAQ)

How much does Hastelloy C-276 plate weigh per square metre?

8.89 × t kg, where t is the thickness in millimetres and 8.89 g/cm³ is the specification density. That gives 26.67 kg/m² at 3 mm, 88.9 kg/m² at 10 mm and 444.5 kg/m² at 50 mm. The figure is exact and repeatable; it is the one number on a plate enquiry nobody can argue with.

Why is thin plate more expensive per kilogram than heavy plate?

Because the conversion cost spreads over less weight and the yield loss is proportionally larger. Rolling to 3 mm needs more passes, flatness control is harder, and trimming and edge defects cost a bigger fraction of a light sheet. Heavy plate is closer to the as-rolled condition, so less of its cost is process.

Does this page publish a price per kilogram?

No. The alloy charge re-prices with the nickel and molybdenum indices, and C-276 carries 15-17 % molybdenum plus 3.0-4.5 % tungsten, both of which trade independently of nickel. A band printed here would be out of date before the plate shipped. The weight table and the cost ordering are stable and are published in full.

How do I turn a plate size into a budget figure?

Multiply the area in square metres by 8.89 × t to get the exact weight, then apply the price your supplier quotes for that thickness, quantity and standard. On plate the input mass is usually close to the finished mass, so the yield question matters less than it does on a machined part.

Why is C-276 more expensive than 316L stainless?

Chemistry first: C-276 specifies 15-17 % molybdenum plus 3.0-4.5 % tungsten against 316L’s 2-3 % molybdenum and no tungsten. Both of those additions trade on their own markets, which is why the gap widens and narrows with molybdenum rather than with nickel. The premium buys chloride and reducing-acid service that 316L cannot hold.

Does the price include certification?

Ask for the certificate level explicitly. EN 10204 3.1 to the heat is the normal basis for this alloy; 3.2 third-party witnessed, PMI on tungsten-bearing heats and additional NDT each add cost and time. None of them are included unless the enquiry says so.