Hastelloy X is chosen for one property above all: oxidation resistance at temperature, verified to a ceiling of 1100 °C in this site’s data. It is a Ni-Cr-Fe-Mo alloy (UNS N06002, GB GH3536, density 8.22 g/cm³) built for gas-turbine combustion chambers, afterburner components and industrial furnace hardware, places where the part sees a hot oxidising gas stream, thermal cycling and, often, carburizing or nitriding atmospheres. The question the grade answers is not “how strong is it at room temperature” but “how long does it resist oxide scale breakdown and environmental attack in the combustion zone”.

What oxidation resistance means at 1100 °C

At high temperature a nickel-chromium alloy survives by growing a protective, adherent chromium-oxide scale that slows further oxidation. The failure modes are spalling (the scale detaches under thermal cycling), breakaway oxidation (the scale stops protecting) and internal attack along grain boundaries. Hastelloy X’s chromium content sustains that protective scale up to a verified 1100 °C, which is why it is the reference material for combustion-zone hardware rather than a higher-strength but lower-chromium grade. Continuous service and cyclic service are different duties: cycling stresses the scale, so the ceiling that matters is the one for your cycle, not the peak figure alone.

Carburization and nitriding

Furnace and reformer atmospheres are not simply oxidising, they can be carburizing (carbon pickup, which embrittles) or nitriding (nitrogen pickup, which hardens and cracks). Hastelloy X is documented on this site as resistant to carburization and nitriding, which is the second reason it holds furnace and petrochemical cracking-tube applications alongside the combustion hardware. Where the atmosphere alternates between oxidising and reducing, state the full gas composition in the enquiry, the material choice can hinge on it.

Where it sits against the other high-temperature grades

Temperature ceiling is the first filter. From the stocked grades on this site:

GradeVerified ceilingCharacter
Hastelloy X1100 °CCombustion-zone oxidation standard
Incoloy 800H1100 °CCreep strength for ASME pressure duty above 600 °C
Inconel 625980 °CSolid-solution strength + corrosion resistance
Waspaloy870 °CAge-hardenable creep-rupture strength
Nimonic 80A815 °Cγ′-strengthened valve alloy

X and 800H share the same ceiling and divide the duty: X for combustion-zone oxidation and mixed furnace atmospheres, 800H for pressure-boundary creep strength with an ASME Section III/VIII basis.

The standards and how to order

Hastelloy X is supplied on this site as bar and rod, plate and sheet, strip, pipe and tube, wire, flange and forging, anchored against AMS 5536, AMS 5754 and ASTM B435 / B572. To order, state: Hastelloy X, UNS N06002 (GB GH3536), the form and its standard (ASTM B435 plate/sheet/strip, ASTM B572 rod/bar, or the AMS number where aerospace applies), the condition (solution annealed), the service atmosphere and temperature, and the certificate (EN 10204 3.1 heat chemistry, or 3.2 witnessed). Use the RFQ spec writer to assemble the enquiry, and the maximum-service-temperature lookup to compare ceilings across the stocked grades.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How oxidation resistant is Hastelloy X?

This site verifies Hastelloy X to a service ceiling of 1100 °C, and documents it as resistant to carburization and nitriding as well as oxidation. It is the reference material for gas-turbine combustion chambers and afterburner components.

Hastelloy X or Incoloy 800H at high temperature?

Both are verified to 1100 °C. Hastelloy X suits combustion-zone oxidation and mixed furnace atmospheres. Incoloy 800H is chosen for ASME Section III/VIII pressure-boundary creep strength above about 600 °C. The duty, not the ceiling alone, decides.

What is the UNS number for Hastelloy X?

UNS N06002 (GB GH3536). It is a Ni-Cr-Fe-Mo alloy with a verified density of 8.22 g/cm³ and oxidation resistance to 1100 °C.

Which standards cover Hastelloy X?

This site anchors Hastelloy X against AMS 5536, AMS 5754, ASTM B435 (plate, sheet, strip) and ASTM B572 (rod, bar). Cite the form standard that matches your product.