1J50 is picked on two numbers from the opposite end of the magnetic-circuit problem to 1J22: initial permeability above 30,000, which lets a small magnetising current set up a large flux, and coercivity below 8 A/m, which lets the flux collapse almost for free when the current is removed. Instrument transformer cores, magnetic amplifier laminations, relay armatures and electromagnetic shielding all live on that pair of figures, 50% Ni-Fe is the verified chemistry behind them.

1J50 is a Chinese soft magnetic alloy (50% Ni-Fe) offering high initial permeability, low coercivity and high saturation induction.

What high permeability and low coercivity buy you

A core with initial permeability above 30,000 needs only a small magnetising force to drive flux, which is what keeps a current transformer’s ratio honest at instrument accuracy. A coercivity below 8 A/m means the core barely resists demagnetisation, so the B-H loop is narrow and the hysteresis loss per cycle stays low, the behaviour magnetic amplifiers and relay armatures are designed around. Both figures are properties of the supplied condition: 1J50 requires high-temperature annealing, and the annealed state is what the numbers assume.

Property1J50 (verified)
Chemistry50% Ni-Fe
Initial permeability> 30,000
Coercivity< 8 A/m
Max service temperature450 °C
Density8.2 g/cm³
Governing standardsGB/T 14986, IEC 60404-8-6
Stock formsWire, Strip, Plate & Sheet, Bar & Rod

Specification signals

The applications map onto the two numbers directly: instrument transformer cores and sensor and transducer cores spend the permeability on measurement accuracy, magnetic amplifier laminations spend the narrow loop on controlled switching, relay and solenoid armatures spend the low coercivity on fast, clean release, and electromagnetic shielding spends the high permeability on diverting stray flux around a sensitive circuit. Strip dominates, laminations and wrapped cores are strip products, with wire, plate and bar for the remaining hardware.

  • Measurement: instrument transformer cores and sensor cores running on the > 30,000 initial permeability
  • Switching and relays: magnetic amplifier laminations and relay armatures using the < 8 A/m coercivity for clean cycling
  • Shielding: enclosures that divert stray flux by giving it a high-permeability path

Where 1J50 stops being the answer

If the circuit must run near saturation, 1J22’s 2.4 T ceiling is the pick and 1J50’s permeability numbers are irrelevant. And the verified figures only hold in the annealed condition, a part machined or formed after annealing moves the properties. Specify 1J50 against GB/T 14986 or IEC 60404-8-6 with the annealing condition on the drawing, and let the certificate prove the chemistry.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

What do 1J50’s permeability and coercivity figures mean in practice?

Initial permeability above 30,000 means a small magnetising current establishes a large flux, and coercivity below 8 A/m means the core demagnetises with almost no opposing field. Together they give the narrow B-H loop that instrument transformers, magnetic amplifiers and shielding are designed around.

Why does 1J50 require high-temperature annealing?

The verified permeability and coercivity are properties of the annealed state. Cold working degrades both, so the datasheet lists high-temperature annealing as a requirement, the final anneal comes after forming, and the condition belongs on the purchase order.

Should I use 1J50 or 1J22 for a magnetic circuit?

Decide on the operating point: circuits that run near saturation need 1J22’s 2.4 T ceiling, and circuits that need high permeability with low loss, transformers, amplifiers, shielding, need 1J50’s > 30,000 / < 8 A/m pair. The two grades answer opposite questions.

Which standard governs a 1J50 order?

GB/T 14986 for the Chinese precision-alloy designation and IEC 60404-8-6 for the international soft-magnetic sheet classification. Cite one explicitly so the mill certificate proves the grade by chemistry against it.