Most buyers arriving with a superalloy bar, plate, strip and pipe forms question about 1J22 need one decision on superalloy bar, plate, strip and pipe forms, not a survey. The verified 1J22 data and the routing logic here close it for good.
1J22: HiperCo 50 equivalent, Fe-Co-V alloy with the highest saturation induction of any soft magnetic material..
As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.
What Superalloy Bar, Plate, Strip and Pipe Forms means for 1J22
What fixes superalloy bar, plate, strip and pipe forms for 1J22 is the verified envelope (8.2 g/cm³, 450 °C) read against solenoid armatures, pole pieces and weight-critical magnetic hardware.
| Property | 1J22 |
|---|---|
| Grade | 1J22 |
| Density | 8.2 g/cm³ |
| Max service temp | 450 °C |
| Best duty | Solenoid armatures, pole pieces and weight-critical magnetic hardware |
| Available forms | Wire, Strip, Plate & Sheet, Bar & Rod |
| Standards | GB/T 14986, AMS 7717 equivalent, ASTM A801 |
Specification signals
Stock does not invent forms, so the purchase order chooses among Wire, Strip, Plate & Sheet, Bar & Rod rather than wishing for another. In practice the applications list confirms the fit: 1J22 is specified for aerospace solenoid armatures and magnetic bearing pole pieces, not as a universal filler.
- One 1J22 datasheet callout does most of the work on this page: Highest saturation induction (2.4 T). A purchasing audit on the 1J22 order checks that line first.
In practice
Stay inside the stocked bands and the quote comes back in days, cross the edge of the range and the mill has to roll to order. Pick the form from the list and let solenoid armatures, pole pieces and weight-critical magnetic hardware sanity-check it.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy bar, plate, strip and pipe forms resolve for 1J22?
Forms come first. Stay inside the stocked bands and the quote comes back in days, cross the edge of the range and the mill has to roll to order.
What is 1J22 best used for?
Solenoid armatures, pole pieces and weight-critical magnetic hardware. The HiperCo 50 equivalent with the highest saturation induction (2.4 T) of any soft magnetic material.
What forms is 1J22 available in?
1J22 ships as Wire, Strip, Plate & Sheet, Bar & Rod, within the stock range of each form.
What standards does 1J22 meet?
Every 1J22 order cites its governing standard (GB/T 14986, AMS 7717 equivalent, ASTM A801) and arrives with an EN 10204 3.1 certificate proving the heat.
When does 1J22 stop being the right choice?
1J22 stops being right above 450 °C, or in media its family was not built for.