Ask a superalloy bar, plate, strip and pipe forms question about Hastelloy C-276 (N10276) and the answer lives in the verified reference data Hastelloy C-276 is built to. This is the practical guide to superalloy bar, plate, strip and pipe forms on Hastelloy C-276, drawn from RAS Thermal’s superalloy documentation.
Hastelloy C-276 (N10276) is a Hastelloy grade whose datasheet leans on one documented property: Resists pitting, crevice and stress-corrosion cracking.
Hastelloy C-276 (N10276) carries a verified composition band of Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5%: the range each element must fall in per the governing standard, and the band the mill certificate cites.
What Superalloy Bar, Plate, Strip and Pipe Forms means for Hastelloy C-276
What fixes superalloy bar, plate, strip and pipe forms for Hastelloy C-276 (N10276) is the verified envelope (8.89 g/cm³, 400 °C) read against chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
| Property | Hastelloy C-276 |
|---|---|
| Grade | Hastelloy C-276 (N10276) |
| Density | 8.89 g/cm³ |
| Max service temp | 400 °C |
| Best duty | Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy |
| Available forms | Forging, Wire, Plate, Sheet, Strip, Bar, Tube |
| Standards | ASTM B575, ASTM B574, ASTM B564, UNS N10276 |
Specification signals
The supplied forms for Hastelloy C-276: Forging, Wire, Plate, Sheet, Strip, Bar, Tube. In practice the applications list confirms the fit: Hastelloy C-276 is specified for chemical reactor internals and flue-gas desulfurization scrubbers, not as a universal filler.
- The feature that separates Hastelloy C-276 from its nearest neighbours is specific: UNS N10276 traceability. Hold the Hastelloy C-276 certificate to proving it, not asserting it.
In practice
Size the part inside the stocked bands (Ø6-350 mm bar, 0.5-80 mm plate, 0.05-3.0 mm strip, 6-219 mm tube OD, 0.10-12.0 mm wire) and lead times stay normal. Form follows the part.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy bar, plate, strip and pipe forms resolve for Hastelloy C-276?
The supplied forms for Hastelloy C-276: Forging, Wire, Plate, Sheet, Strip, Bar, Tube. Within the standard ranges (bar and rod Ø6-350 mm, plate and sheet 0.5-80 mm, strip 0.05-3.0 mm, pipe and tube OD 6-219 mm, wire Ø0.10-12.0 mm) the form choice follows the machined part, not the alloy.
What is Hastelloy C-276 best used for?
Hastelloy C-276 is stocked for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy; the documented edge is that the general-purpose Ni-Cr-Mo corrosion grade for aggressive wet service, weldable without post-weld heat treatment.
What forms is Hastelloy C-276 available in?
Stocked forms: Forging, Wire, Plate, Sheet, Strip, Bar, Tube.
What standards does Hastelloy C-276 meet?
ASTM B575, ASTM B574, ASTM B564, UNS N10276 are the standards Hastelloy C-276 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Hastelloy C-276 stop being the right choice?
The ceiling is 400 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.