Most buyers arriving with a superalloy bar, plate, strip and pipe forms question about Hastelloy X (N06002) need one decision on superalloy bar, plate, strip and pipe forms, not a survey. The verified Hastelloy X data and the routing logic here close it for good.

Hastelloy X (N06002): Ni-Cr-Fe-Mo alloy for combustion zone components with exceptional oxidation resistance to 1100°C..

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What Superalloy Bar, Plate, Strip and Pipe Forms means for Hastelloy X

Hastelloy X (N06002) on superalloy bar, plate, strip and pipe forms: density 8.22 g/cm³, verified ceiling 1100 °C. The deciding facts are temperature, media and form, and they land on gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.

PropertyHastelloy X
GradeHastelloy X (N06002) · GB GH3536
Density8.22 g/cm³
Max service temp1100 °C
Best dutyGas turbine combustion chambers, afterburners and furnace hardware above 1000 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube
StandardsAMS 5536, AMS 5754, ASTM B435, ASTM B572

Specification signals

The supplied forms for Hastelloy X: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. In practice the applications list confirms the fit: Hastelloy X is specified for gas turbine combustion chambers and afterburner components, not as a universal filler.

  • The feature that separates Hastelloy X from its nearest neighbours is specific: Combustion zone standard material. Hold the Hastelloy X certificate to proving it, not asserting it.

In practice

Lead time is a geometry decision. One list, one order.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy bar, plate, strip and pipe forms resolve for Hastelloy X?

Stock does not invent forms, so the purchase order chooses among Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube rather than wishing for another. Lead time is a geometry decision.

What is Hastelloy X best used for?

Hastelloy X is stocked for gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C; the documented edge is that the combustion-zone standard, oxidation resistant to 1100 °C with good fabricability.

What forms is Hastelloy X available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Hastelloy X meet?

Hastelloy X ships against AMS 5536, AMS 5754, ASTM B435, ASTM B572 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Hastelloy X stop being the right choice?

The ceiling is 1100 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.