Ask a superalloy bar, plate, strip and pipe forms question about Incoloy 800 (N08800) and the answer lives in the verified reference data Incoloy 800 is built to. This is the practical guide to superalloy bar, plate, strip and pipe forms on Incoloy 800, drawn from RAS Thermal’s superalloy documentation.

Incoloy 800 (N08800) is a Incoloy grade whose datasheet leans on one documented property: Cost-effective vs Inconel.

For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.

What Superalloy Bar, Plate, Strip and Pipe Forms means for Incoloy 800

For Incoloy 800 (N08800), superalloy bar, plate, strip and pipe forms comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

PropertyIncoloy 800
GradeIncoloy 800 (N08800) · GB NS111
Density7.94 g/cm³
Max service temp1100 °C
Best dutyPetrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASTM B408, ASME SB-407

Specification signals

Pick from the list Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, because Incoloy 800 only gets certified in the forms it is actually stocked in. In practice the applications list confirms the fit: Incoloy 800 is specified for ethylene furnace tubes and heat exchanger bundles, not as a universal filler.

  • The feature that separates Incoloy 800 from its nearest neighbours is specific: Carburization and nitriding resistant. Hold the Incoloy 800 certificate to proving it, not asserting it.

In practice

Designers who size sections against the 0.10-12.0 mm wire and 0.05-3.0 mm strip bands before drawing lock in normal delivery instead of a special roll. petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C fails on paper long before it fails in service if the chosen form cannot be certified.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy bar, plate, strip and pipe forms resolve for Incoloy 800?

Incoloy 800 is stocked as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, and that list is what the purchase order picks from. Stay inside the stocked bands and the quote comes back in days, cross the edge of the range and the mill has to roll to order.

What is Incoloy 800 best used for?

Incoloy 800 is stocked for petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C; the documented edge is that the cost-effective Ni-Fe-Cr workhorse for furnace tubes and heat exchangers, oxidation and carburization resistant to 1100 °C.

What forms is Incoloy 800 available in?

Stocked forms: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube.

What standards does Incoloy 800 meet?

Every Incoloy 800 order cites its governing standard (ASTM B163, ASTM B407, ASTM B408, ASME SB-407) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Incoloy 800 stop being the right choice?

The ceiling is 1100 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.