Ask a superalloy bar, plate, strip and pipe forms question about Inconel 718 (N07718) and the answer lives in the verified reference data Inconel 718 is built to. This is the practical guide to superalloy bar, plate, strip and pipe forms on Inconel 718, drawn from RAS Thermal’s superalloy documentation.
Inconel 718 (N07718) is a Inconel alloy rated to 650 °C, stocked for Turbine discs and rings.
Inconel 718 (N07718) is bought to a composition band of Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%; both the governing standard and the mill certificate are read against it.
What Superalloy Bar, Plate, Strip and Pipe Forms means for Inconel 718
What fixes superalloy bar, plate, strip and pipe forms for Inconel 718 (N07718) is the verified envelope (8.19 g/cm³, 650 °C) read against rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
| Property | Inconel 718 |
|---|---|
| Grade | Inconel 718 (N07718) |
| Density | 8.19 g/cm³ |
| Max service temp | 650 °C |
| Best duty | Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C |
| Available forms | Forging, Wire, Spring Wire, Bar, Plate, Strip |
| Standards | AMS 5662, AMS 5663, ASTM B637, UNS N07718 |
Specification signals
For Inconel 718, the semi-finished stock forms are Forging, Wire, Spring Wire, Bar, Plate, Strip. In practice the applications list confirms the fit: Inconel 718 is specified for turbine discs and rings and compressor blades and fasteners, not as a universal filler.
- One Inconel 718 datasheet callout does most of the work on this page: AMS 5662 / 5663 rotating-quality certified. A purchasing audit on the Inconel 718 order checks that line first.
In practice
Part geometry picks the form. Form follows the part.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy bar, plate, strip and pipe forms resolve for Inconel 718?
Every enquiry for Inconel 718 starts by matching the drawing to one of Forging, Wire, Spring Wire, Bar, Plate, Strip, and a form off the list means a mill quote. Lead time is a geometry decision.
What is Inconel 718 best used for?
Inconel 718 is stocked for rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C; the documented edge is that the precipitation-hardened workhorse for turbine discs and fasteners, age-hardened to 38 HRC with usable strength to 650 °C.
What forms is Inconel 718 available in?
Stocked forms: Forging, Wire, Spring Wire, Bar, Plate, Strip.
What standards does Inconel 718 meet?
Every Inconel 718 order cites its governing standard (AMS 5662, AMS 5663, ASTM B637, UNS N07718) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Inconel 718 stop being the right choice?
Inconel 718 stops being right above 650 °C, or in media its family was not built for.