Ask a superalloy bar, plate, strip and pipe forms question about L605 (R30605) and the answer lives in the verified reference data L605 is built to. This is the practical guide to superalloy bar, plate, strip and pipe forms on L605, drawn from RAS Thermal’s superalloy documentation.

L605 (R30605) is a Cobalt-Based alloy rated to 980 °C, stocked for Aerospace bearing races and rings.

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Bar, Plate, Strip and Pipe Forms means for L605

What fixes superalloy bar, plate, strip and pipe forms for L605 (R30605) is the verified envelope (9.13 g/cm³, 980 °C) read against aerospace bearing races, wear rings and combustion hardware.

PropertyL605
GradeL605 (R30605) · GB GH605
Density9.13 g/cm³
Max service temp980 °C
Best dutyAerospace bearing races, wear rings and combustion hardware
Available formsForging, Wire, Bar & Rod
StandardsAMS 5759, AMS 5537, ASTM F90

Specification signals

Every enquiry for L605 starts by matching the drawing to one of Forging, Wire, Bar & Rod, and a form off the list means a mill quote. In practice the applications list confirms the fit: L605 is specified for aerospace bearing races and rings and gas turbine wear components, not as a universal filler.

  • One L605 datasheet callout does most of the work on this page: Excellent wear and galling resistance. A purchasing audit on the L605 order checks that line first.

In practice

Stock envelopes to plan against: bar Ø6-350 mm, plate 0.5-80 mm, strip 0.05-3.0 mm, tube OD 6-219 mm, wire to Ø12.0 mm. Sizes outside them are mill-quote territory. Pick the form from the list and let aerospace bearing races, wear rings and combustion hardware sanity-check it.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy bar, plate, strip and pipe forms resolve for L605?

Every enquiry for L605 starts by matching the drawing to one of Forging, Wire, Bar & Rod, and a form off the list means a mill quote. Lead time is a geometry decision.

What is L605 best used for?

Aerospace bearing races, wear rings and combustion hardware, which is where this grade’s datasheet numbers are actually verified.

What forms is L605 available in?

L605 ships as Forging, Wire, Bar & Rod, within the stock range of each form.

What standards does L605 meet?

Every L605 order cites its governing standard (AMS 5759, AMS 5537, ASTM F90) and arrives with an EN 10204 3.1 certificate proving the heat.

When does L605 stop being the right choice?

The ceiling is 980 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.