What MP35N (R30035) can and cannot do on superalloy bar, plate, strip and pipe forms is fixed by the verified envelope below. Datasheet facts on MP35N, and the decision they drive for superalloy bar, plate, strip and pipe forms. Nothing else.
MP35N (R30035): Co-Ni-Cr-Mo alloy with ultra-high tensile strength, fatigue endurance and biocompatibility..
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What Superalloy Bar, Plate, Strip and Pipe Forms means for MP35N
What fixes superalloy bar, plate, strip and pipe forms for MP35N (R30035) is the verified envelope (8.43 g/cm³, 425 °C) read against medical implants, aerospace fasteners and high-performance springs.
| Property | MP35N |
|---|---|
| Grade | MP35N (R30035) |
| Density | 8.43 g/cm³ |
| Max service temp | 425 °C |
| Best duty | Medical implants, aerospace fasteners and high-performance springs |
| Available forms | Forging, Wire, Spring Wire, Bar & Rod, Strip |
| Standards | ASTM F562, AMS 5844, AMS 5845, ISO 5832-6 |
Specification signals
The list is short on purpose. The documented applications tell the same story (medical implants and guidewires, aerospace fasteners), and a duty outside that list deserves a second look before MP35N goes on the order.
- The feature that separates MP35N from its nearest neighbours is specific: Ultra-high tensile strength (>1800 MPa achievable). Hold the MP35N certificate to proving it, not asserting it.
In practice
Stock envelopes to plan against: bar Ø6-350 mm, plate 0.5-80 mm, strip 0.05-3.0 mm, tube OD 6-219 mm, wire to Ø12.0 mm. Sizes outside them are mill-quote territory. One list, one order.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy bar, plate, strip and pipe forms resolve for MP35N?
For MP35N, the semi-finished stock forms are Forging, Wire, Spring Wire, Bar & Rod, Strip. Stock envelopes to plan against: bar Ø6-350 mm, plate 0.5-80 mm, strip 0.05-3.0 mm, tube OD 6-219 mm, wire to Ø12.0 mm. Sizes outside them are mill-quote territory.
What is MP35N best used for?
Medical implants, aerospace fasteners and high-performance springs, which is where this grade’s datasheet numbers are actually verified.
What forms is MP35N available in?
Stocked forms: Forging, Wire, Spring Wire, Bar & Rod, Strip.
What standards does MP35N meet?
Every MP35N order cites its governing standard (ASTM F562, AMS 5844, AMS 5845, ISO 5832-6) and arrives with an EN 10204 3.1 certificate proving the heat.
When does MP35N stop being the right choice?
Two things end it: a peak service temperature above 425 °C, or media outside the family MP35N was built for.