Most buyers arriving with a superalloy bar, plate, strip and pipe forms question about Nickel 200 (N02200) need one decision on superalloy bar, plate, strip and pipe forms, not a survey. The verified Nickel 200 data and the routing logic here close it for good.

Nickel 200 is a commercially pure wrought nickel (99.6% minimum) offering excellent corrosion resistance in caustic alkalis, synthetic fiber production and food processing.

As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.

What Superalloy Bar, Plate, Strip and Pipe Forms means for Nickel 200

For Nickel 200 (N02200), superalloy bar, plate, strip and pipe forms comes down to the documented envelope: 8.89 g/cm³, 315 °C ceiling, and a duty best described as caustic soda evaporator tubes, spinnerets and electrical terminals.

PropertyNickel 200
GradeNickel 200 (N02200) · GB N6
Density8.89 g/cm³
Max service temp315 °C
Best dutyCaustic soda evaporator tubes, spinnerets and electrical terminals
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B160, ASTM B161, ASTM B162, ASME SB-160

Specification signals

Stock does not invent forms, so the purchase order chooses among Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube rather than wishing for another. The documented applications tell the same story (caustic soda evaporator tubes, synthetic fiber spinnerets), and a duty outside that list deserves a second look before Nickel 200 goes on the order.

  • One Nickel 200 datasheet callout does most of the work on this page: Excellent caustic alkali resistance. A purchasing audit on the Nickel 200 order checks that line first.

In practice

Within the standard ranges (bar and rod Ø6-350 mm, plate and sheet 0.5-80 mm, strip 0.05-3.0 mm, pipe and tube OD 6-219 mm, wire Ø0.10-12.0 mm) the form choice follows the machined part, not the alloy. Forms serve the part. caustic soda evaporator tubes, spinnerets and electrical terminals tells you which part.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy bar, plate, strip and pipe forms resolve for Nickel 200?

Nickel 200 is stocked as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, and that list is what the purchase order picks from. Part geometry picks the form.

What is Nickel 200 best used for?

Nickel 200 is stocked for caustic soda evaporator tubes, spinnerets and electrical terminals; the documented edge is that commercially pure wrought nickel (99.6% min) for caustic alkalis and electrical duty.

What forms is Nickel 200 available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Nickel 200 meet?

ASTM B160, ASTM B161, ASTM B162, ASME SB-160 are the standards Nickel 200 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.

When does Nickel 200 stop being the right choice?

Two things end it: a peak service temperature above 315 °C, or media outside the family Nickel 200 was built for.