Ask a superalloy maximum service temperature question about Hastelloy X (N06002) and the answer lives in the verified reference data Hastelloy X is built to. This is the specification guide to superalloy maximum service temperature on Hastelloy X, drawn from RAS Thermal’s superalloy documentation.

Hastelloy X (N06002): Ni-Cr-Fe-Mo alloy for combustion zone components with exceptional oxidation resistance to 1100°C..

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Maximum Service Temperature means for Hastelloy X

What fixes superalloy maximum service temperature for Hastelloy X (N06002) is the verified envelope (8.22 g/cm³, 1100 °C) read against gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.

PropertyHastelloy X
GradeHastelloy X (N06002) · GB GH3536
Density8.22 g/cm³
Max service temp1100 °C
Best dutyGas turbine combustion chambers, afterburners and furnace hardware above 1000 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube
StandardsAMS 5536, AMS 5754, ASTM B435, ASTM B572

Specification signals

The verified ceiling for Hastelloy X reads 1100 °C. Not a rule of thumb, the datasheet figure. The documented applications tell the same story (gas turbine combustion chambers, afterburner components), and a duty outside that list deserves a second look before Hastelloy X goes on the order.

  • One Hastelloy X datasheet callout does most of the work on this page: Resistant to carburization and nitriding. A purchasing audit on the Hastelloy X order checks that line first.

In practice

Margin has a price. Everything above 1100 °C is a different conversation, and gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C never asks for it.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy maximum service temperature resolve for Hastelloy X?

Check the temperature axis first: Hastelloy X verifies to 1100 °C, and the envelope ends exactly there. Excursions are the trap.

What is Hastelloy X best used for?

Gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Hastelloy X available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Hastelloy X meet?

Every Hastelloy X order cites its governing standard (AMS 5536, AMS 5754, ASTM B435, ASTM B572) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Hastelloy X stop being the right choice?

The ceiling is 1100 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.