Ask a superalloy maximum service temperature question about Incoloy 800 (N08800) and the answer lives in the verified reference data Incoloy 800 is built to. This is the specification guide to superalloy maximum service temperature on Incoloy 800, drawn from RAS Thermal’s superalloy documentation.

Incoloy 800 is an iron-nickel-chromium alloy with good strength and oxidation/carburization resistance at high temperatures.

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Maximum Service Temperature means for Incoloy 800

What fixes superalloy maximum service temperature for Incoloy 800 (N08800) is the verified envelope (7.94 g/cm³, 1100 °C) read against petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

PropertyIncoloy 800
GradeIncoloy 800 (N08800) · GB NS111
Density7.94 g/cm³
Max service temp1100 °C
Best dutyPetrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASTM B408, ASME SB-407

Specification signals

Run the peak continuous temperature past 1100 °C and Incoloy 800 is no longer the grade on the certificate, whatever the brochure implies. In practice the applications list confirms the fit: Incoloy 800 is specified for ethylene furnace tubes and heat exchanger bundles, not as a universal filler.

  • The feature that separates Incoloy 800 from its nearest neighbours is specific: ASME code approved. Hold the Incoloy 800 certificate to proving it, not asserting it.

In practice

Treat 1100 °C as a wall, not a target, and the duty list writes itself once the real peak is measured. Everything above 1100 °C is a different conversation, and petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C never asks for it.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy maximum service temperature resolve for Incoloy 800?

Run the peak continuous temperature past 1100 °C and Incoloy 800 is no longer the grade on the certificate, whatever the brochure implies. Margin has a price.

What is Incoloy 800 best used for?

Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C. The cost-effective Ni-Fe-Cr workhorse for furnace tubes and heat exchangers, oxidation and carburization resistant to 1100 °C.

What forms is Incoloy 800 available in?

Incoloy 800 ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.

What standards does Incoloy 800 meet?

Every Incoloy 800 order cites its governing standard (ASTM B163, ASTM B407, ASTM B408, ASME SB-407) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Incoloy 800 stop being the right choice?

Incoloy 800 stops being right above 1100 °C, or in media its family was not built for.