Superalloy Maximum Service Temperature, applied to Incoloy 800H (N08810): verified numbers first, then the reasoning a specifier applies to Incoloy 800H. A RAS Thermal reference page on superalloy maximum service temperature.
Incoloy 800H (N08810) is a Incoloy grade whose datasheet leans on one documented property: Enhanced creep strength vs 800.
As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.
What Superalloy Maximum Service Temperature means for Incoloy 800H
Incoloy 800H (N08810) on superalloy maximum service temperature: density 7.94 g/cm³, verified ceiling 1100 °C. The deciding facts are temperature, media and form, and they land on ASME pressure vessels, steam methane reformers and power plant superheaters.
| Property | Incoloy 800H |
|---|---|
| Grade | Incoloy 800H (N08810) · GB NS1102 |
| Density | 7.94 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | ASME pressure vessels, steam methane reformers and power plant superheaters |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII |
Specification signals
Run the peak continuous temperature past 1100 °C and Incoloy 800H is no longer the grade on the certificate, whatever the brochure implies. In practice the applications list confirms the fit: Incoloy 800H is specified for asme pressure vessels and high-temperature heat exchangers, not as a universal filler.
- One Incoloy 800H datasheet callout does most of the work on this page: Good structural stability. A purchasing audit on the Incoloy 800H order checks that line first.
In practice
Incoloy 800H’s own feature list says the same thing in plainer words: Superior to 800 above 600°C. Set the duty list honestly and Incoloy 800H holds that ceiling across ASME pressure vessels, steam methane reformers and power plant superheaters.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy maximum service temperature resolve for Incoloy 800H?
Incoloy 800H is rated to 1100 °C. That ceiling is verified, and it is the number the datasheet and the certificate must both hold. Excursions are the trap.
What is Incoloy 800H best used for?
Incoloy 800H is stocked for ASME pressure vessels, steam methane reformers and power plant superheaters; the documented edge is that the controlled-carbon 800 variant with enhanced creep strength for ASME pressure vessel duty above 600 °C.
What forms is Incoloy 800H available in?
The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.
What standards does Incoloy 800H meet?
ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII are the standards Incoloy 800H is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Incoloy 800H stop being the right choice?
Incoloy 800H stops being right above 1100 °C, or in media its family was not built for.