Superalloy Maximum Service Temperature, applied to Inconel 718 (N07718): verified numbers first, then the reasoning a specifier applies to Inconel 718. A RAS Thermal reference page on superalloy maximum service temperature.
Inconel 718 (N07718) is a Inconel alloy rated to 650 °C, stocked for Turbine discs and rings.
The verified composition band for Inconel 718 (N07718) is Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%; that band is what the mill certificate is checked against, element by element.
What Superalloy Maximum Service Temperature means for Inconel 718
Inconel 718 (N07718) on superalloy maximum service temperature: density 8.19 g/cm³, verified ceiling 650 °C. The deciding facts are temperature, media and form, and they land on rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
| Property | Inconel 718 |
|---|---|
| Grade | Inconel 718 (N07718) |
| Density | 8.19 g/cm³ |
| Max service temp | 650 °C |
| Best duty | Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C |
| Available forms | Forging, Wire, Spring Wire, Bar, Plate, Strip |
| Standards | AMS 5662, AMS 5663, ASTM B637, UNS N07718 |
Specification signals
Inconel 718 is rated to 650 °C. That ceiling is verified, and it is the number the datasheet and the certificate must both hold. In practice the applications list confirms the fit: Inconel 718 is specified for turbine discs and rings and compressor blades and fasteners, not as a universal filler.
- The feature that separates Inconel 718 from its nearest neighbours is specific: Excellent fabricability and weldability. Hold the Inconel 718 certificate to proving it, not asserting it.
In practice
Excursions are the trap. Hold the peak under 650 °C and Inconel 718 keeps the promise written into rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy maximum service temperature resolve for Inconel 718?
Heat decides first. Treat 650 °C as a wall, not a target, and the duty list writes itself once the real peak is measured.
What is Inconel 718 best used for?
Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C. The precipitation-hardened workhorse for turbine discs and fasteners, age-hardened to 38 HRC with usable strength to 650 °C.
What forms is Inconel 718 available in?
Inconel 718 ships as Forging, Wire, Spring Wire, Bar, Plate, Strip, within the stock range of each form.
What standards does Inconel 718 meet?
Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Inconel 718 stop being the right choice?
The ceiling is 650 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.