Superalloy Maximum Service Temperature, applied to Waspaloy (N07001): verified numbers first, then the reasoning a specifier applies to Waspaloy. A RAS Thermal reference page on superalloy maximum service temperature.
Waspaloy (N07001) is a Waspaloy grade whose datasheet leans on one documented property: Exceptional creep-rupture strength to 870°C.
As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.
What Superalloy Maximum Service Temperature means for Waspaloy
For Waspaloy (N07001), superalloy maximum service temperature comes down to the documented envelope: 8.22 g/cm³, 870 °C ceiling, and a duty best described as turbine discs, rings, shafts and high-temperature fasteners.
| Property | Waspaloy |
|---|---|
| Grade | Waspaloy (N07001) · GB GH4738 |
| Density | 8.22 g/cm³ |
| Max service temp | 870 °C |
| Best duty | Turbine discs, rings, shafts and high-temperature fasteners |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip |
| Standards | AMS 5708, AMS 5709, AMS 5544, ASTM B637 |
Specification signals
At 870 °C, the certificate and the datasheet still agree, and that agreement is the whole reason the part gets specified. The documented applications tell the same story (turbine discs and rings, compressor shafts), and a duty outside that list deserves a second look before Waspaloy goes on the order.
- One Waspaloy datasheet callout does most of the work on this page: Microstructural stability under thermal cycling. A purchasing audit on the Waspaloy order checks that line first.
In practice
Peak matters more than average, because a short trip over 870 °C costs the guarantee that long steady running below it never touched. So the temperature question closes first.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy maximum service temperature resolve for Waspaloy?
The verified ceiling for Waspaloy reads 870 °C. Not a rule of thumb, the datasheet figure. Treat 870 °C as a wall, not a target, and the duty list writes itself once the real peak is measured.
What is Waspaloy best used for?
Turbine discs, rings, shafts and high-temperature fasteners, which is where this grade’s datasheet numbers are actually verified.
What forms is Waspaloy available in?
Waspaloy ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, within the stock range of each form.
What standards does Waspaloy meet?
AMS 5708, AMS 5709, AMS 5544, ASTM B637 are the standards Waspaloy is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Waspaloy stop being the right choice?
The ceiling is 870 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.