Ask a superalloy spring wire selection question about Inconel 718 (N07718) and the answer lives in the verified reference data Inconel 718 is built to. This is the specification guide to superalloy spring wire selection on Inconel 718, drawn from RAS Thermal’s superalloy documentation.
Inconel 718 (N07718) is a Inconel grade whose datasheet leans on one documented property: Precipitation-hardenable to 38 HRC.
Inconel 718 (N07718) carries a verified composition band of Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%: the range each element must fall in per the governing standard, and the band the mill certificate cites.
What Superalloy Spring Wire Selection means for Inconel 718
Inconel 718 (N07718) on superalloy spring wire selection: density 8.19 g/cm³, verified ceiling 650 °C. The deciding facts are temperature, media and form, and they land on rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
| Property | Inconel 718 |
|---|---|
| Grade | Inconel 718 (N07718) |
| Density | 8.19 g/cm³ |
| Max service temp | 650 °C |
| Best duty | Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C |
| Available forms | Forging, Wire, Spring Wire, Bar, Plate, Strip |
| Standards | AMS 5662, AMS 5663, ASTM B637, UNS N07718 |
Specification signals
Inconel 718 is one of the spring-wire grades (Inconel 718 | X-750 | 625 | C-276 | A-286 | Monel K-500 | MP35N | 3J21). In practice the applications list confirms the fit: Inconel 718 is specified for turbine discs and rings and compressor blades and fasteners, not as a universal filler.
- The feature that separates Inconel 718 from its nearest neighbours is specific: Cryogenic to 650°C service. Hold the Inconel 718 certificate to proving it, not asserting it.
In practice
Wire form means temper selection is the real decision. The draw and the temper carry the fatigue story, and the certificate states both. That is the role rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C plays at wire gauge.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy spring wire selection resolve for Inconel 718?
Being named inside (Inconel 718 | X-750 | 625 | C-276 | A-286 | Monel K-500 | MP35N | 3J21) means Inconel 718 can be ordered in cold-drawn spring temper without a special qualification argument. Temper is the real decision.
What is Inconel 718 best used for?
Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C. The precipitation-hardened workhorse for turbine discs and fasteners, age-hardened to 38 HRC with usable strength to 650 °C.
What forms is Inconel 718 available in?
The stocked forms are Forging, Wire, Spring Wire, Bar, Plate, Strip; sizes follow the stock range for the form you pick.
What standards does Inconel 718 meet?
Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Inconel 718 stop being the right choice?
Two things end it: a peak service temperature above 650 °C, or media outside the family Inconel 718 was built for.