ASTM B160 covers nickel rod and bar, on this site, Nickel 200 (UNS N02200), the commercially pure wrought nickel with 99.6% minimum nickel content. Caustic soda evaporator hardware, synthetic-fibre spinnerets, electrical terminals and food-processing equipment are the verified applications, and B160 is the bar standard the machined versions are bought against.

A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.

What the standard covers

The grade is chosen on purity, not strength. Nickel 200 (GB N6, 8.89 g/cm³) verifies excellent caustic alkali resistance, high electrical and thermal conductivity, non-magnetic behaviour and food-grade qualification, with service to 315 °C. Where the duty is corrosion in caustic media or conduction rather than high temperature or load, it is the reference grade. The form rules the document: bar and rod sit under B160, while pipe and flat product carry their own designations.

Grades under this standard

ItemVerified detail
AlloyNickel 200 (UNS N02200, GB N6)
Purity99.6% minimum nickel
Density8.89 g/cm³
Max service temperature315 °C
Form pairingB160 rod/bar · B161 pipe/tube · B162 plate/sheet/strip

How to order against it

Order B160 by UNS, form and condition (hot rolled, forged, cold drawn, peeled or ground are the bar states). For caustic equipment state the media on the PO, and for electrical hardware state the conductivity requirement. EN 10204 3.1 with heat chemistry, and the 99.6% minimum purity it proves, is the acceptance basis.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Which alloy does ASTM B160 cover?

Nickel 200, UNS N02200, commercially pure wrought nickel at 99.6% minimum, in rod and bar. Its pipe is B161 and its flat product is B162.

Why choose Nickel 200 over Monel 400 in caustic service?

Purity. At 99.6% minimum nickel, Nickel 200 is the reference grade for caustic soda equipment, and Monel 400 adds copper for seawater and HF duty. The medium picks the grade.

Does B160 material conduct electricity well?

Yes, high electrical and thermal conductivity are verified key features of commercially pure nickel, which is why electrical lead wires and terminals are listed applications.