ASTM B435 is the sheet-and-plate home of Hastelloy X on this site: the alloy that lives in the flame path, combustor cans, afterburner sections, furnace interiors running past 1000 °C, is bought as B435 flat product. GH3044 (N06604) joins it, citing B435-equivalent supply for Chinese-system hot-section sheet work.
A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What the standard covers
The page divides along two procurement systems. Hastelloy X (N06002, GB GH3536, 8.22 g/cm³) is the Western combustion-zone answer: it shrugs off oxidation to 1100 °C, resists carburization and nitriding in fuel-rich atmospheres, and forms well enough that engine and furnace sheet fabrications are routine. GH3044 (N06604, 8.89 g/cm³, GB/T 14994) is the Ni-Cr-W Chinese answer for the same class of sheet parts, rated to 900 °C and certified B435-equivalent. Choose by specification system first, then by the 200 °C gap in verified ceilings.
Grades under this standard
| Grade | UNS / GB | Density | Max service temp | Standards cited |
|---|---|---|---|---|
| Hastelloy X | N06002 / GH3536 | 8.22 g/cm³ | 1100 °C | ASTM B435, B572, AMS 5536, AMS 5754 |
| GH3044 | N06604 / GB/T 14994 | 8.89 g/cm³ | 900 °C | GB/T 14994, ASTM B435 equivalent |
How to order against it
Buy B435 flat product in the solution-annealed state, sized against the stocked range, plate and sheet to 80 mm, strip from 0.05 mm. Aerospace call-outs stack AMS 5536 on top of B435, and GB-system projects order GH3044 to GB/T 14994 with the B435-equivalent note on the certificate. Either way the EN 10204 3.1 heat chemistry is the acceptance document.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
Which grades ship under ASTM B435?
Hastelloy X (N06002) is the primary grade, with GH3044 (N06604) citing B435-equivalent supply for its furnace and hot-section sheet duty.
Is B435 only for aerospace?
No, industrial furnace hardware is equally within scope. Hastelloy X’s verified applications span gas turbine combustion chambers, afterburners, industrial furnace hardware and heat-treating equipment.
How does B435 relate to AMS 5536?
B435 is the ASTM flat-product specification, and AMS 5536 is the aerospace sheet specification for the same alloy. Cite both when the hardware flies, B435 alone for industrial duty.