ASTM B443 is the plate, sheet and strip specification for one alloy this site stocks: Inconel 625, UNS N06625. When a pressure vessel, heat-exchanger shell or chemical-equipment liner is drawn in 625 flat product, B443 is the standard the certificate cites, and the strip end of its range is what bellows and diaphragm makers buy.

A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.

What the standard covers

The alloy itself explains the specification’s job: Inconel 625 is a solid-solution Ni-Cr-Mo grade with verified pitting and crevice-corrosion resistance, oxidation resistance to 980 °C, non-magnetic behaviour and excellent weldability, the reason it appears in seawater piping, chemical processing equipment and aircraft ducting. B443 pins the flat-product forms: plate and sheet for vessel and exchanger construction, strip down to thin gauges for formed components. That form-to-standard mapping earns its keep the moment a purchase order spans several product shapes at once, mismatched citations are how certificates and drawings drift apart.

Grades under this standard

ItemVerified detail
AlloyInconel 625 (UNS N06625, GB GH3625)
Product forms under B443Plate, sheet, strip
Companion standardsB446 (bar & rod), B444 (pipe & tube)
Density8.44 g/cm³
Max service temperature980 °C
Key dutyPitting/crevice resistance, sour service (NACE MR0175)

How to order against it

Specify B443 by alloy, UNS, form and condition, solution annealed is the normal supply state for corrosion duty. Site stock ranges matter for planning: plate and sheet 0.5-80 mm thick, strip 0.05-3.0 mm at 4-600 mm width. Require EN 10204 3.1 with heat-specific chemistry, and where the service is sour, add NACE MR0175 to the call-out.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Which alloy does ASTM B443 cover?

Inconel 625, UNS N06625, in plate, sheet and strip. The same alloy in bar and rod is B446 and in seamless pipe and tube is B444, the form decides the standard.

What thickness range is available under B443?

Site stock runs plate and sheet from 0.5 to 80 mm and strip from 0.05 to 3.0 mm in widths to 600 mm, the thin end is what formed bellows and diaphragm components consume.

Is Inconel 625 plate weldable per B443 supply condition?

Yes, excellent weldability is a verified key feature of the alloy, and solution-annealed flat product is the standard supply state for welded vessel and piping construction.