ASTM B575 is the plate, sheet and strip specification for the low-carbon nickel-molybdenum-chromium family, in site terms, the Hastelloy C line: the legacy Hastelloy C, C-4, C-22 and the workhorse C-276. Reactor internals, FGD scrubber shell sections and bleach equipment are fabricated from B575 flat product, and the alloy choice inside the family is a media-and-fabrication decision.
A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What the standard covers
Read the family by chemistry and generation. Hastelloy C-276 (N10276, 8.89 g/cm³) is the general-purpose wet-corrosion armour, verified against pitting, crevice attack and stress-corrosion cracking across a wide acid range, weldable without post-weld heat treatment, rated to 400 °C. C-22 (N06022, 8.69 g/cm³) trades toward superior oxidizing-media resistance and better weldability than C-276. C-4 (N06455, 8.64 g/cm³) is the high-temperature-stable grade free of intergranular precipitation. The legacy Hastelloy C (GB NS3303, 8.94 g/cm³) remains for general wet-corrosion service where the modern variants are not specified. All four roll to the same flat-product scope: plate and sheet form vessel shells, strip feeds formed internals.
Grades under this standard
| Grade | UNS / GB | Density | Max service temp | Standout duty |
|---|---|---|---|---|
| Hastelloy C-276 | N10276 | 8.89 g/cm³ | 400 °C | Broadest acid resistance, no PWHT |
| Hastelloy C-22 | N06022 | 8.69 g/cm³ | 600 °C | Oxidizing media, better weldability |
| Hastelloy C-4 | N06455 | 8.64 g/cm³ | 600 °C | Intergranular-precipitation-free stability |
| Hastelloy C | NS3303 (GB) | 8.94 g/cm³ | 600 °C | Legacy general wet corrosion |
How to order against it
Purchasing B575 material is a chemistry-first exercise: pick the C-family variant by the actual liquor chemistry, name the UNS on the order, and demand heat-specific OES proof so the low-carbon guarantee is documented rather than assumed. Bar stock for these grades travels under ASTM B574, say so explicitly when the PO covers both forms. For scrubber and sour duties, write the media into the purchase line so the variant choice is on record.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
Which grades does ASTM B575 cover on this site?
Four Hastelloy C-family grades cite it for plate, sheet and strip: C-276, C-22, C-4 and the legacy Hastelloy C. Bar for the same grades is ASTM B574.
C-276 or C-22 for an FGD scrubber?
C-276 is the broadest verified shield across reducing and oxidizing acids, and C-22 pushes further into oxidizing media with better weldability. The scrubber’s actual liquor chemistry decides, both ship under B575.
Does B575 material need post-weld heat treatment?
Not for C-276, good weldability without post-weld heat treatment is a verified key feature, and the low-carbon family chemistry is what makes as-welded vessel construction viable.