Superalloy Standards (ASTM, AMS, GB/T), applied to Hastelloy C-276 (N10276): verified numbers first, then the reasoning a specifier applies to Hastelloy C-276. A RAS Thermal reference page on superalloy standards (astm, ams, gb/t).
Hastelloy C-276 (N10276) is a Hastelloy grade whose datasheet leans on one documented property: Resists pitting, crevice and stress-corrosion cracking.
Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5% is the certified band for Hastelloy C-276 (N10276): every element bounded by the governing standard and proven on the certificate rather than assumed.
What Superalloy Standards (ASTM, AMS, GB/T) means for Hastelloy C-276
For Hastelloy C-276 (N10276), superalloy standards (astm, ams, gb/t) comes down to the documented envelope: 8.89 g/cm³, 400 °C ceiling, and a duty best described as chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
| Property | Hastelloy C-276 |
|---|---|
| Grade | Hastelloy C-276 (N10276) |
| Density | 8.89 g/cm³ |
| Max service temp | 400 °C |
| Best duty | Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy |
| Available forms | Forging, Wire, Plate, Sheet, Strip, Bar, Tube |
| Standards | ASTM B575, ASTM B574, ASTM B564, UNS N10276 |
Specification signals
Those documents are the grade’s spine. The documented applications tell the same story (chemical reactor internals, flue-gas desulfurization scrubbers), and a duty outside that list deserves a second look before Hastelloy C-276 goes on the order.
- The feature that separates Hastelloy C-276 from its nearest neighbours is specific: UNS N10276 traceability. Hold the Hastelloy C-276 certificate to proving it, not asserting it.
In practice
Cite the standard and the UNS together. A designation without its document is how certificates and drawings drift apart. Every shipment for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy cites the same governing documents, which is what keeps multi-batch builds interchangeable.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy standards (astm, ams, gb/t) resolve for Hastelloy C-276?
A purchase order for Hastelloy C-276 can cite ASTM B575, ASTM B574, ASTM B564, UNS N10276, and no other document is needed to name the grade. Rejecting the wrong document at goods-in is cheap, discovering it after fabrication is not, so the citation is checked first.
What is Hastelloy C-276 best used for?
Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy, which is where this grade’s datasheet numbers are actually verified.
What forms is Hastelloy C-276 available in?
The stocked forms are Forging, Wire, Plate, Sheet, Strip, Bar, Tube; sizes follow the stock range for the form you pick.
What standards does Hastelloy C-276 meet?
Hastelloy C-276 ships against ASTM B575, ASTM B574, ASTM B564, UNS N10276 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Hastelloy C-276 stop being the right choice?
The ceiling is 400 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.