What Hastelloy X (N06002) can and cannot do on superalloy standards (astm, ams, gb/t) is fixed by the verified envelope below. Datasheet facts on Hastelloy X, and the decision they drive for superalloy standards (astm, ams, gb/t). Nothing else.

Hastelloy X (N06002): Ni-Cr-Fe-Mo alloy for combustion zone components with exceptional oxidation resistance to 1100°C..

For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.

What Superalloy Standards (ASTM, AMS, GB/T) means for Hastelloy X

For Hastelloy X (N06002), superalloy standards (astm, ams, gb/t) comes down to the documented envelope: 8.22 g/cm³, 1100 °C ceiling, and a duty best described as gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.

PropertyHastelloy X
GradeHastelloy X (N06002) · GB GH3536
Density8.22 g/cm³
Max service temp1100 °C
Best dutyGas turbine combustion chambers, afterburners and furnace hardware above 1000 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube
StandardsAMS 5536, AMS 5754, ASTM B435, ASTM B572

Specification signals

The ladder runs AMS 5536, AMS 5754, ASTM B435, ASTM B572 with GH3536 as the domestic mirror, and every rung is auditable. In practice the applications list confirms the fit: Hastelloy X is specified for gas turbine combustion chambers and afterburner components, not as a universal filler.

  • One Hastelloy X datasheet callout does most of the work on this page: Combustion zone standard material. A purchasing audit on the Hastelloy X order checks that line first.

In practice

Standards are the audit trail. Name the one that governs, and reject certificates that cite something else. Paperwork travels with the part.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy standards (astm, ams, gb/t) resolve for Hastelloy X?

Calling out AMS 5536, AMS 5754, ASTM B435, ASTM B572 alongside GB GH3536 is how a drawing tells the mill exactly what Hastelloy X has to meet. A certificate that answers to a different designation than the AMS 5536 callout on the drawing is a rejection, not a clerical difference.

What is Hastelloy X best used for?

Hastelloy X is stocked for gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C; the documented edge is that the combustion-zone standard, oxidation resistant to 1100 °C with good fabricability.

What forms is Hastelloy X available in?

Hastelloy X ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube, within the stock range of each form.

What standards does Hastelloy X meet?

Every Hastelloy X order cites its governing standard (AMS 5536, AMS 5754, ASTM B435, ASTM B572) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Hastelloy X stop being the right choice?

The ceiling is 1100 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.