Most buyers arriving with a superalloy standards (astm, ams, gb/t) question about Incoloy 800 (N08800) need one decision on superalloy standards (astm, ams, gb/t), not a survey. The verified Incoloy 800 data and the routing logic here close it for good.

Incoloy 800 (N08800) is a Incoloy alloy rated to 1100 °C, stocked for Ethylene furnace tubes.

As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.

What Superalloy Standards (ASTM, AMS, GB/T) means for Incoloy 800

Incoloy 800 (N08800) on superalloy standards (astm, ams, gb/t): density 7.94 g/cm³, verified ceiling 1100 °C. The deciding facts are temperature, media and form, and they land on petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

PropertyIncoloy 800
GradeIncoloy 800 (N08800) · GB NS111
Density7.94 g/cm³
Max service temp1100 °C
Best dutyPetrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASTM B408, ASME SB-407

Specification signals

Name the document, name the grade. The documented applications tell the same story (ethylene furnace tubes, heat exchanger bundles), and a duty outside that list deserves a second look before Incoloy 800 goes on the order.

  • One Incoloy 800 datasheet callout does most of the work on this page: Good creep-rupture strength. A purchasing audit on the Incoloy 800 order checks that line first.

In practice

Chemistry, properties, test method, one document. Every shipment for petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C cites the same governing documents, which is what keeps multi-batch builds interchangeable.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy standards (astm, ams, gb/t) resolve for Incoloy 800?

The standards ladder for Incoloy 800: ASTM B163, ASTM B407, ASTM B408, ASME SB-407, GB NS111. Drift starts with vague callouts.

What is Incoloy 800 best used for?

Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Incoloy 800 available in?

Stocked forms: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube.

What standards does Incoloy 800 meet?

Incoloy 800 ships against ASTM B163, ASTM B407, ASTM B408, ASME SB-407 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Incoloy 800 stop being the right choice?

Incoloy 800 stops being right above 1100 °C, or in media its family was not built for.